Measuring elastic property of single-walled carbon nanotubes by nanoindentation: A theoretical framework
Mechanics Research Communications(2008)
摘要
Nanoindentation is an effective technique for deducing the elastic property of single-walled carbon nanotubes (SWCNTs). Following an atomistic study of the nanoindentation mechanism, reverse analysis algorithms are proposed by utilizing the indentation force-depth data measured from the initial uniaxial compression and post-buckling regimes, respectively, which lead to stretching stiffness of 382Pam and 429Pam, that are very close to those in the literature. Parallel finite element simulations incorporating atomic interactions are also carried out, which closely duplicates the indentation response of SWCNTs in atomistic simulations. The numerical studies carried out in this paper may be used to guide the nanoindentation experiments, explain and extract useful data from the test, as well as stimulate new experiments.
更多查看译文
关键词
Nanoindentation,Carbon nanotube,Elastic property,Molecular mechanics
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要