Barium titanate films were synthesized by anodic oxidation galvanostatically in an electrolyte of 0.5 M Ba(CH3COO)2 with 2 M NaOH. The films were first prepared using a wide constant current range from 5 to 40 mA. XRD results showed that rutile TiO2 was present at 10 mA and cubic BaTiO3 films could be obtained at currents over 20 mA. The Ti anodes were then electrolyzed at constant current of 30 mA with various deposition times from 0.5 to 4 h. XRD results showed that TiO2 existed at 0.5 h and BaTiO3 appeared at electrolytic times over 0.75 h. From the XRD results associated with the variations of electrolytic voltage with time, rutile TiO2 has been found to be a precursor for the formation of BaTiO3. BaTiO3 films with uniformly distributed small grains were formed at voltages over 60 V and below the dielectric breakdown voltage. The formation mechanism could be due to dissolution and crystallization. BaTiO3 films with large crater shaped grains were present when voltages reached a dielectric breakdown voltage, which could be due to anodic spark deposition.
更多
查看译文
关键词
Barium titanate,Anodising,X-Ray diffraction,SEM,Anodic spark deposition
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
0
您的评分 :

暂无评分

数据免责声明
页面数据均来自互联网公开来源、合作出版商和通过AI技术自动分析结果,我们不对页面数据的有效性、准确性、正确性、可靠性、完整性和及时性做出任何承诺和保证。若有疑问,可以通过电子邮件方式联系我们:report@aminer.cn