High Growth Rate of Erbium Oxide Thin Films in Atomic Layer Deposition from (CpMe)3Er and Water Precursors

CHEMICAL VAPOR DEPOSITION, no. 10 (2005): 415.0-419

Cited by: 52|Views1
Get fulltext within 24h
Bibtex

Abstract

Organometallic tris(methylcyclopentadienyl)erbium and water were successfully exploited as precursors for the atomic layer deposition (ALD) of Er2O3 thin films. Deposition studies were carried out in the temperature range 175-450 degrees C, where Si(100) and soda-lime glass were used as substrates. ALD-type growth mechanism could be verif...More