Recovery of Iron from Hematite‐Rich Diasporic‐Type Bauxite Ore

6TH INTERNATIONAL SYMPOSIUM ON HIGH-TEMPERATURE METALLURGICAL PROCESSING(2015)

引用 0|浏览11
暂无评分
摘要
A technique has been proposed for recovering iron from hematite-rich diasporic-type bauxite ore in this study. Direct reduction roasting followed by low intensity wet magnetic separation process was carried out. The parameters including reduction temperature and time, sodium salts, grinding conditions and magnetic field intensity for separation of iron were determined. The optimum process parameters as follows: roasting temperature of 1050 degrees C, time of 60 min, sodium salts involving sodium sulfate, borax, sodium carbonate with dosages of 10 wt%, 2 wt%, 35 wt% respectively, and magnetic field intensity of 1000 Gs with fineness of pulp reached 92.75% passing -0.074mm. Under the optimal conditions, an iron concentrate containing 88.17% total iron grade and iron recovery of 92.51% was obtained, 4.55% total iron grade in tailings. This novel technique provide a potential route for utilizing hematite-rich diasporic bauxite ore, recovering iron resource firstly, and extracting alumina from magnetic separation tailings further.
更多
查看译文
关键词
Diasporic bauxite, Sodium salts, DRI, Magnetic separation, Alumina
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要