•Fabrication of adiabatic foam using sodium silicate and glass fiber.•Thermal conductivity is about 0.0454–0.0459W/mK.•Density is about 74–80kg/m3 and compression strength is about 0.42–0.46MPa.•Thermal conductivity is more sensitive to glass fiber content.