摘要
•A system for automatic visual monitoring of welding process is introduced.•It deals with monitoring of welding in dry stainless steel kegs for food storage.•5 kinds of defects are taken into consideration.•It can work in critical conditions (inside the kegs).•it does not use structured light making exploitable miniaturized hardware for data acquisition.•Inspection performances have been evaluated by using a large set of kegs.
更多查看译文
关键词
Non-invasive inspection,Monitoring production process,Inspection for welding procedure,Non destructive testing,Stainless steel kegs,Food storage