The effect of crack path on tearing resistance of a narrow-gap Alloy 52 dissimilar metal weld

Engineering Fracture Mechanics(2018)

引用 11|浏览2
暂无评分
摘要
•HAZ cracks can deviate from the initial crack growth plane to the fusion boundary.•The J-R curves are smallest for cracks initiating at the fusion boundary.•The 10 × 10 and 10 × 20 SE(B) specimens yield similar J-R curves.
更多
查看译文
关键词
Tearing resistance,Crack path,Dissimilar metal weld,Strength mismatch,Nuclear power plant