Hysteresis And Domain Behaviors Analysis Of High Purity Fe-(5,6) Wt% Si Alloys

20TH INTERNATIONAL CONFERENCE ON MAGNETISM, ICM 2015(2015)

引用 0|浏览3
暂无评分
摘要
We investigated the improvement in magnetic properties of high-purity Fe-(5, 6) wt% Si formed by cold crucible levitation melting. The results showed that Fe-6 wt% Si alloy has a smaller coercivity than Fe-5 wt% Si. The hysteresis loss of both alloys increases linearly and slightly with maximum magnetization, and increases significantly after a certain maximum magnetization. Additionally, demagnetized domain structure and domain wall motion in both samples was studied by means of Lorentz microscopy. The results indicated that the domain wall motion of Fe-6 wt% Si can be activated in lower external fields and displaces more rapidly than Fe-5 wt% Si. Moreover, the displacement of domain walls that penetrate symmetrical grain boundaries and dislocations in Fe-6 wt% Si was analyzed. The boundaries and dislocations have no pinning effect on domain wall motion.
更多
查看译文
关键词
Fe-(5,6)wt% Si, Lorentz microscopy, Magnetic domain
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要