Comparison of short and long term creep testing in high performance polymers
Polymer Testing(2019)
摘要
The creep behaviour of thermoplastics plays an important role in engineering design and especially the failure and lifetime prediction of structural components in a variety of industries. Often this mechanical property is determined with long-term creep tests. In order to reduce the development time of components made from such materials used in applications with conditions over 100 °C for long times, we propose the use of dynamic-mechanical analysis to predict long-term creep deformation through the stepped isothermal (SIM) and the stepped isostress methods (SSM). The present study aims to determine whether SIM and SSM can be generalised to material characterisation of advanced polymers at high temperature. Both methods are evaluated and verified by long-term measurements. Both amorphous and semi-crystalline polymers are studied and the influence of the glass transition temperature (Tg) on the accelerated test results is examined with tests conducted above and below the Tg region for PEEK. The results of our analysis show accelerated testing is an effective tool in predicting long term behaviour and comparing the creep response of thermoplastics. PAI exhibits a far superior creep response when compared to PEEK and PEI over 100 °C.
更多查看译文
关键词
Creep behaviour,Time-temperature superposition,Time-stress superposition,Dynamic-mechanical analysis,Stepped isothermal method,Stepped isostress method
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要