Fretting fatigue damage mechanism of Nickel-based single crystal superalloys at high temperature

International Journal of Mechanical Sciences(2020)

引用 20|浏览4
暂无评分
摘要
•A novel high temperature fretting fatigue test apparatus has been developed.•Surface peeling, delamination and micro cracks occur due to fretting fatigue.•Fretting fatigue cracks initiate on the contact leading edge and grow along slip plane.•Fretting fatigue damage mechanism considering fretting wear and crystallographic was proposed.
更多
查看译文
关键词
Fretting fatigue,Nickel-based single crystal,Fretting wear,Crystallographic slip