Methodology improvement of bulk compressive creep test: Deformation measurement and loading rate
Dental Materials(2022)
摘要
The accuracy of deformation measurement during bulk compressive creep test could be improved by means of introducing stainless steel hemisphere to the loading chain, and adding preload process to loading protocol.
更多查看译文
关键词
Viscoelastic,Bulk compressive creep test,Resin composite,Deformation measurement,Loading rate