Oxidation of Silicon Carbide Composites for Nuclear Applications at Very High Temperatures in Steam

COATINGS(2022)

引用 5|浏览2
暂无评分
摘要
Single-rod oxidation and quench experiments at very high temperatures in steam atmosphere were conducted with advanced, nuclear grade SiCf/SiC CMC cladding tube segments. A transient experiment was performed until severe local degradation of the sample at maximum temperature of approximately 1845 degrees C. The degradation was caused by complete consumption of the external CVD-SiC sealcoat, resulting in steam access to the fiber-matrix composite with less corrosion resistance. Approaching these very high temperatures was accompanied by accelerated gas release mainly of H-2 and CO2, the formation of surface bubbles and white smoke. Three one-hour isothermal tests at 1700 degrees C in steam with final water flooding and one three-hour experiment with fast cool-down in Ar atmosphere were run under nominally identical conditions. All isothermally tested samples survived the tests without any macroscopic degradation. The mechanical performance of these quenched clad segments was not significantly affected, while maintaining a high capability to tolerate damages. Despite these harsh exposure conditions, load transfer between SiC fibers and matrix remained efficient, allowing the composites to accommodate deformation.
更多
查看译文
关键词
silicon carbide, ceramic matrix composite, nuclear fuel cladding, high-temperature oxidation, water steam, mechanical properties
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要