Study on Corrosion, Hydrogen Permeation and Stress Corrosion Cracking Behavior of Aisi 4135 Steel in the Marine Tidal Zone
SSRN Electronic Journal(2022)
关键词
stress corrosion cracking behavior,stress corrosion,hydrogen permeation,steel