Analysis of Differential Scanning Calorimetry (DSC): Determining the Transition Temperatures, and Enthalpy and Heat Capacity Changes in Multicomponent Systems by Analytical Model Fitting
Journal of thermal analysis and calorimetry(2023)
摘要
We have developed an analytical method to quantitatively analyze differential scanning calorimetry (DSC) experimental data. This method provides accurate determination of thermal properties such as equilibrium melting temperature, latent heat, change of heat capacity which can be performed automatically without intervention of a DSC operator. DSC is one of the best techniques to determine the thermal properties of materials. However, the accuracy of the transition temperature and enthalpy change can be affected by artifacts caused by the instrumentation, sampling, and the DSC analysis methods which are based on graphical constructions. In the present study, an analytical function (DSC N (T)) has been developed based on an assumed Arrhenius crystal size distribution together with instrumental and sample-related peak broadening. The DSC N (T) function was successfully applied to fit the experimental data of a substantial number of calibration and new unknown samples, including samples with an obvious asymmetry of the melting peak, yielding the thermal characteristics such as melting and glass transition temperature, and enthalpy and heat capacity change. It also allows very accurate analysis of binary systems with two distinct but severely overlapping peaks and samples that include a cold crystallization before melting.
更多查看译文
关键词
DSC,Analytical function,Melting temperature,Glass transition,Crystallization,Change in heat capacity and enthalpy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要