The Role of Nitrogen Gas and PWHT on Pitting Corrosion Behavior of Duplex Stainless-Steel Joint Made by GTAW
Metallography Microstructure and Analysis(2024)
Key words
Duplex stainless steel,Welding,Nitrogen gas,Pitting corrosion,Microstructure