Abstract This paper presents a comprehensive parametric analysis and optimization of friction stir welding (FSW) for dissimilar joining of additively manufactured nanocomposites: polylactic acid reinforced with TiO 2 nanoparticles (PLA/TiO 2 ) and polyether ether ketone reinforced with carbon nanotubes (PEEK/CNT). The main focus is to evaluate the effects of welding parameters – rotation speed, traverse speed, and tool tilt angle – on the flexural strength and elastic modulus of the welded joints. The experiments were designed using the Taguchi method, and the grey relational analysis (GRA) technique was used to determine the optimal conditions for maximizing both flexural strength and elastic modulus. Signal to noise (S/N) analysis revealed that rotation speed exerts the most significant influence on both flexural strength and elastic modulus, followed by traverse speed. The optimal parameter combination was 1,500 rpm rotation speed, 10 mm/s traverse speed, and 2° tilt angle, under which elastic modulus and flexural strength improved by 11 % and 32 %, respectively. Under these optimized settings, the welded joint achieved 80 % of the elastic modulus and 75 % of the flexural strength of the weaker base nanocomposite (PLA/TiO 2 ). Microstructural analysis confirmed that adequate heat input at 1,500 rpm promoted smooth flow lines and a dense, defect-free interface, while excessive speed (2,000 rpm) induced void formation and particle detachment. This research conclusively demonstrates that FSW is a viable and effective technique for producing high-performance hybrid joints between biodegradable PLA-based and high-strength PEEK-based nanocomposites, with significant potential for advanced biomedical and structural engineering applications requiring tailored stiffness and bending resistance.
Abstract Epoxy composites are widely used in industries such as construction, automobile, marine and aerospace. These composites are cost-effective, environment friendly, and have good strength while considering their weight. However, since their strength is not enough compared to conventional materials used in several industrial applications, it would be noteworthy to develop a composite with improved performance. In this investigation an effort was made to manufacture composites using two different fibers, guava and Indian cork. Composites were developed using the conventional hand layup procedure. Two different types of composites containing tri-layers were prepared, G/I/G (Guava/Indian cork/Guava) and I/G/I (Indian cork/Guava/Indian cork). Their Mechanical strength was assessed by conducting tensile, flexural and impact tests. Results revealed that G/I/G composite exhibited higher strength due to the higher strength of guava fiber and its double concentration relative to Indian cork fiber. In addition, the G/I/G composite was reinforced with silica particles with different quantities and its performance was assessed. G/I/G-2wt% silica composite recorded maximum (Tensile: 55 MPa; flexural: 70 MPa; Impact: 10.2 kJ/m2; hardness: 82 Shore D). Further more, the G/I/G-3wt% silica composite exhibited the least water uptake. Thus, the present research promotes that G/I/G-2wt% composite is suitable material for construction, automobile, and marine applications.
Abstract In this study, ternary blends of polyamide 66/polyamide 610/polyamide 12 (PA66/PA610/PA12) were firstly prepared, and exhibited the best mechanical performance when the mass ratio of PA610 to PA12 was 2:3 and their total content was 20 wt%. On this basis, the ternary blend was mixed with glass fiber (GF), brominated polystyrene/antimony trioxide (BS) to prepare a PA66 composite (PA66/610/12/BS/GF), and the samples without long chain polyamides and flame retardants (PA66/BS/GF and PA66/610/12/GF) were also prepared for comparison. DSC and XRD analyses showed that PA610 was immiscible with PA66 after short-time blending. Besides, long-chain polyamides (PA610 and PA12) and flame retardants, especially Sb 2 O 3 , increased the crystallinity ( X c ) of PA66 in the composites, leading to the highest X c of PA66 in PA66/610/12/BS/GF. SEM images revealed that BPS was dispersed in the polyamide matrix at a microscale size. Mechanical tests revealed that long-chain polyamides and flame retardants exhibited a synergistic effect, which could simultaneously enhance the strength and toughness of PA66/GF, and promote its charring reaction and char residue yield. In addition, all the composites containing flame retardants showed excellent flame retardancy, reaching the UL-94 V-0 rating. Therefore, PA66/610/12/BS/GF is a composite with UL-94 V-0 flame retardancy, high strength, high toughness and good thermal stability, and can be used for components requiring high comprehensive performance in the electrical and electronic, automotive and home appliance fields.
Abstract Fiber diameter and defect-free morphology, particularly the suppression of bead formation, are critical to the performance of electrospun fibers. This study employs complementary physicochemical and rheological approaches to predict fiber morphology using poly(butylene succinate) (PBS) dissolved in a DMF–chloroform solvent blend, with poly(methyl methacrylate) (PMMA) incorporated in selected samples. Guided by Colby’s theory, specific viscosity measurements identified 6.067 % PBS as the minimum concentration for fiber formation and 21 % PBS as the concentration producing uniform, defect-free fibers, while the critical entanglement concentration (Ce) was determined from specific viscosity. From a rheological perspective, the interactions among electrical, elastic, and capillary forces were analyzed using Feng’s Slender Body model, which yielded results consistent with Yu and Fridrikh’s formulations while avoiding reliance on imaging-derived jet parameters. The specific-viscosity-based approach provided predictions with relatively low error margins of approximately 2–5 % compared with more complex rheological methods. Although the model slightly overestimated fiber morphology parameters, it provides a practical approach for predicting electrospinning outcomes and defect formation.
The present work involved the surface modification of waste coffee grounds (WCG) via cold plasma using Ar as the precursor gas. The untreated and plasma-treated WCG particles were mixed with high-density polyethylene (HDPE) at a 20/80 wt% ratio of filler to polymer by using a two-roll mill followed by a hydraulic press. The effect of plasma surface treatment on the performance of composites was investigated using various analytical techniques, including tensile and izod impact strength tests, thermogravimetric analysis (TGA), contact profilometry analysis, density measurements, and scanning electron microscopy (SEM). The incorporation of WCG resulted in a reduction in both the impact strength and tensile strength of the composite material. Nevertheless, plasma surface treatment resulted in significant improvements in both impact strength and tensile strength compared to WCG composites that had not been subjected to cold plasma. The TGA results demonstrated that cold plasma treatment increased the thermal stability of WCG/HDPE composites, as the onset temperature of decomposition of plasma-treated WCG composites was higher than that of untreated WCG composites. The SEM images revealed modifications at the fiber-matrix interface, corroborating the improved mechanical properties after treatment with cold plasma. The contact profilometry analysis showed an enhancement in surface roughness, affirming the effect of plasma treatment on the WCG surface. These findings suggest that cold plasma can be utilized as an effective method for the modification of agro-waste materials and the production of high-performance, eco-friendly composite materials.