
In this study, ZnS1−xSex alloys were deposited by RF magnetron co-sputtering with varying ZnSe/ZnS ratios, followed by post-annealing in Ar-H2 at 300 °C. Structure and optoelectronic properties were evaluated. X-ray diffraction revealed that films crystallize in the cubic phase with high (111) orientation, along the 0 < x < 1 composition range indicating the formation of the pseudobinary alloy. UV-Vis spectroscopy confirmed the pseudobinary alloy formation with tunable bandgaps (3.57–2.74 eV) due to Se by S substitution. Tauc plots and Urbach tail parameter showed evidence of electronic states within the bandgap and disorder related to the different ion size in the substitutional alloy. Raman spectroscopy indicates that films have Zn–Se, Zn–S, S–Se bonds in the local-range ordering possibly due to the nature of co-sputtering method. The presence of Zn interstitials was evidenced by the Auger Zn L3M4.5M4 peak at ca. 494 eV from XPS. Photoluminescence in ZnSe revealed the presence of Zni, VZn, VSe, and VZn-VSe defects; in ZnS, the dominant defects were Zni and VS, while VSe and VZn-VSe defects predominate in the films with higher Se contents. Electrochemical impedance spectroscopy indicates a high sheet resistance of the films, while Mott–Schottky plots confirm n-type conductivity in all the films. Semiempirical band diagrams were built using experimental and reported data, indicating that films have a favorable bandgap and band positions for eventual photocatalytic H2 production; however, defects near the valence band could be deleterious for the potential application in photoelectrochemical cells and deserve further consideration.
Atomic layer controlled molybdenum (Mo) etching was performed at <100 °C using alternating exposures of O2 and HCl combined with simultaneous electron exposures and positive sample voltage. Electron exposures at ∼100 eV were derived from a hollow cathode plasma electron source. The Mo surface was oxidized to MoOx using concurrent O2 and electron beam exposures. The Mo oxidation rate increased dramatically when a positive voltage of +20 V was applied to the sample stage. Subsequently, the MoOx layer was linearly etched during synchronous HCl and electron exposures when a positive voltage of +20 V was also applied to the sample stage. No enhancement of the oxidation or etching was observed with a negative voltage of −20 V on the sample stage. The oxidation and etching enhancement in the presence of the positive sample voltage suggested that low energy electrons or anions dominated the reaction. The primary electrons at ∼100 eV can produce low energy electrons by ionization of Ar in the reactor and also by secondary electron yield from the Mo substrate. Low energy electrons can form O− or Cl− anions via dissociative electron attachment. Low energy electrons and anions can then be pulled to the sample stage at +20 V. Alternating oxidation and chlorination steps were applied in a digital fashion to define the Mo etching process. An etch per cycle of 1.3 Å/cycle was measured using in situ spectroscopic ellipsometry. The ellipsometric measurements could separately measure the MoOx growth, MoOx removal, and Mo film thickness loss during each etching cycle.
CuAl2 layers are deposited on MgO(001) substrates by ultrahigh vacuum dc magnetron cosputtering to explore the epitaxial growth of the tetragonal θ-CuAl2 intermetallic compound. Increasing the deposition temperature from Ts = 100 to 400 °C causes a transition from 110- to 001-oriented films, with a pure 110-oriented two-domain epitaxy for Ts = 100 °C, a polycrystalline microstructure for Ts = 200 °C, and epitaxial single crystals with CuAl2(001) || MgO(001) and CuAl2[110] || MgO[100] for Ts ≥ 300 °C. The measured resistivity ρ of d = 350 nm thick layers decreases with increasing Ts = 100–400 °C from 8.14 to 6.39 μΩ cm at 298 K and from 1.92 to 1.35 μΩ cm at 77 K. However, layers with a smaller d = 50 nm exhibit coalesced microstructures with rough surfaces for Ts ≤ 250 °C and discontinuous microstructures for Ts ≥ 300 °C, leading to high effective film resistances. The overall results provide insight into the epitaxial growth of an intermetallic compound, demonstrating epitaxy of the tetragonal θ-CuAl2 phase but also revealing challenges in achieving continuous θ-CuAl2 films which, in turn, prohibit direct measurement of the intrinsic resistivity size effect.
Two-dimensional transition metal dichalcogenides are promising for next-generation technologies due to their unique optical and electronic properties. Tungsten diselenide (WSe2) is especially attractive because of its ambipolar conductivity and high theoretical carrier mobility. However, conventional high-temperature chemical vapor deposition limits WSe2 growth on 3D nanostructured or thermally sensitive substrates. Atomic layer deposition (ALD) could enable large-area, conformal WSe2 synthesis at back-end-of-line compatible temperatures, though it remains underexplored for this material. In this work, we develop and characterize a plasma-enhanced ALD process for 2D layered WSe2 using bis(tert-butylimido)bis(dimethylamino)tungsten as the precursor and pure H2Se plasma as the coreactant at 300 °C. Surface saturation conditions for the precursor and coreactant were established using atomic force microscopy. At 300 and 400 °C, a growth rate of ∼0.3 Å/ALD cycle was obtained. An 8-in wafer map of films deposited at 300 °C demonstrates high thickness uniformity and process scalability. 10 nm thick films grown at both 300 and 400 °C are characterized using Raman, grazing-incidence XRD, XPS, AFM, and SEM. As deposited, the films are crystalline, stoichiometric, and have rough surface morphologies. Cross-sectional STEM and energy-dispersive x-ray spectroscopy indicate crystalline 2D WSe2 layers that are aligned parallel to the surface. Some large amorphous tungsten selenide features are also present, likely caused by selenium contamination and related secondary-deposition processes in the reaction chamber.
To enhance the surface wear resistance of 2Cr12MoV steel and improve its service life, TiC/Al composite coating was fabricated on the surface of 2Cr12MoV steel using the CO2 laser cladding system. The effect of laser power on the coating was investigated. The microstructure, hardness, phase composition, and wear resistance of the cladding layer under different laser powers were studied. The results showed that the phase composition of the composite coating consisted of an Fe0.75Al0.25 metal compound, a Ti-Cr solid solution, TiC, and an Fe-Cr solid solution. As the laser power increases, the average hardness of the composite coating was approximately 1.6–1.7 times than the substrate, but excessive power would lead to a decrease in coating hardness, which was due to the substrate dilution effect and grain coarsening. Moreover, the wear resistance of the coating was also improved. The wear rate of the coating under a power of 1400 W was the lowest [7.47 × 10−6 mm3/(N m)]. The wear mechanism of the coating mainly included fatigue wear, oxidation wear, and abrasive wear.