AbstractCitation analysis of a certain publication acknowledges its impact on the scientific community. This study conducted a multivariate analysis of the top 50 most cited articles published on the field of Bioactive Glass. A systemic search was performed using the “All database” section of the Web of Science to retrieve the top 50 most cited original publications. The selected articles were then manually cross-matched with Elsevier Scopus and Google Scholar Database. Parameters such as article title, authorship, institution, country of publication, year, citation count, citation density, current citation index, and journal name were retrieved from Web of Science. Different ranges of citation numbers were retrieved for these publications in which 197-913 are from Web of Science, 209-962 are from Elsevier Scopus, and 269-1225 are from Google Scholar. A total of 153 authors contributed to this marked list, where Professor L.L. Hench contributed the highest number of articles (n=21). Imperial College London published the highest number of articles (n=21). In summary, this study provides a good scientometric picture of bioactive glass related publications, which illustrate the trend of biomaterials development over the years and suggests future scopes to the scientific community.
AbstractOver the last years, three-dimensional (3D) printing has been successfully applied to produce suitable substitutes for treating bone defects. In this work, 3D printed composite scaffolds of polycaprolactone (PCL) and strontium (Sr)- and cobalt (Co)-doped multi-component melt-derived bioactive glasses (BGs) were prepared for bone tissue engineering strategies. For this purpose, 30% of as-prepared BG particles (size <38 μm) were incorporated into PCL, and then the obtained composite mix was introduced into a 3D printing machine to fabricate layer-by-layer porous structures with the size of 12 × 12 × 2 mm3.The scaffolds were fully characterized through a series of physico-chemical and biological assays. Adding the BGs to PCL led to an improvement in the compressive strength of the fabricated scaffolds and increased their hydrophilicity. Furthermore, the PCL/BG scaffolds showed apatite-forming ability (i.e., bioactivity behavior) after being immersed in simulated body fluid (SBF). The in vitro cellular examinations revealed the cytocompatibility of the scaffolds and confirmed them as suitable substrates for the adhesion and proliferation of MG-63 osteosarcoma cells. In conclusion, 3D printed composite scaffolds made of PCL and Sr- and Co-doped BGs might be potentially-beneficial bone replacements, and the achieved results motivate further research on these materials.
Abstract Porosity is known to play a pivotal role in dictating the functional properties of biomedical scaffolds, with special reference to mechanical performance. While compressive strength is relatively easy to be experimentally assessed even for brittle ceramic and glass foams, elastic properties are much more difficult to be reliably estimated. Therefore, describing and, hence, predicting the relationship between porosity and elastic properties based only on the constitutive parameters of the solid material is still a challenge. In this work, we quantitatively compare the predictive capability of a set of different models in describing, over a wide range of porosity, the elastic modulus (7 models), shear modulus (3 models) and Poisson’s ratio (7 models) of bioactive silicate glass-derived scaffolds produced by foam replication. For these types of biomedical materials, the porosity dependence of elastic and shear moduli follows a second-order power-law approximation, whereas the relationship between porosity and Poisson’s ratio is well fitted by a linear equation.
AbstractThis study investigates the role of yttrium in phosphate-based glasses in the system 45(P2O5)–25(CaO)– (30-x)(Na2O)–x(Y2O3) (0≤x≤5) prepared via melt quenching and focuses on their structural characterisation and degradation properties. The structural analyses were performed using a combination of solid-state nuclear magnetic resonance (NMR), Fourier transform infrared spectroscopy (FTIR) and X-ray photoelectron spectroscopy (XPS). 31P NMR analysis showed that depolymerisation of the phosphate network occurred which increased with Y2O3 content as metaphosphate units (Q2) decreased with subsequent increase in pyrophosphate species (Q1). The NMR results correlated well with structural changes observed via FTIR and XPS analyses. XRD analysis of crystallised glass samples revealed the presence of calcium pyrophosphate (Ca2P2O7) and sodium metaphosphate (NaPO3) phases for all the glass formulations explored. Yttrium-containing phases were found for the formulations containing 3 and 5 mol% Y2O3. Degradation analyses performed in Phosphate buffer saline (PBS) and Milli-Q water revealed significantly reduced rates with addition of Y2O3 content. This decrease was attributed to the formation of Y-O-P bonds where the octahedral structure of yttrium (YO6) cross-linked phosphate chains, subsequently leading to an increase in chemical durability of the glasses. The ion release studies also showed good correlation with the degradation profiles.
AbstractIn this study, injectable pastes based on a clinically-tested bioactive glass and glycerol (used as organic carrier) were produced and characterized for further application in regenerative medicine. The paste preparation route, apatite-forming ability in simulated body fluid (SBF) solution, viscoelastic behavior and structural features revealed by means of scanning electron microscopy (SEM), FTIR and Raman spectroscopy were presented and discussed, also on the basis of the major experimental data obtained in previous studies. A mechanism illustrating the chemical interaction between bioactive glass and glycerol was proposed to support the bioactivity mechanism of injectable pastes. Then, the results of In vivo tests, conducted through injecting moldable paste into osseous defects made in rabbit’s femur, were reported. Animal studies revealed good osteoconductivity and bone bonding that occurred initially at the interface between the glass and the host bone, and further supported the suitability of these bioactive glass pastes in bone regenerative medicine.