Transactions of the Japan Society of Mechanical Engineers. C(2003)
被引用2|浏览1
摘要
Two types of electroforming techniques that can produce thick electroformed coatings were developed to utilize the coatings as microgrinding tools. Sedimented abrasive grains on the cathode were agitated continuously at a low speed to increase the nickel ion density near the cathode when the low-speed agitation technique was employed. In addition, an open space 3 mm square and 15 mm in length was grooved on a cylindrical aclylic insulator that covered the columnar anode, and an attempt to fill the space with the deposited coating was made by rotating the cathode at a low speed when the low-speed rotation technique was employed. It became obvious that an electric force line was concentrated at the edge of the cathode, so that a coating with uniform thickness could not be realized when the low-speed agitation technique was employed. 0n the other hand, high-speed electroforming that can produce a thick coating 3 mm square and 15 mm in length in 18.3 hours was accomplished when the low-speed rotation technique was employed.