It has been shown in this chapter that the MTDSC technique is a very useful tool in the study of several aspects of polymer
blends and related materials including structured latexes and interpenetrating polymer networks. It is important to note that
the dC
p/dT versus temperature signal may be used not only qualitatively as a sensitive detector of transitions impossible to spot by
other thermal techniques such as conventional DSC and DMTA, but it may also be used to significant advantage in a quantitative
way. It has been shown that it is sensitive to the diffuse interface between phases. Thus, from dC
p/dT versus temperature signals, the weight fraction of the diffuse interface can be quantified. There are many situations where
this will prove to be very valuable.