The uniform and compact n-type TiO2 window layers were prepared by RF sputtering using a TiO2 ceramic target. A high open circuit voltage of about 1.03 V with the efficiency of 13.23% can be obtained as compared to 0.92 V of solution based TiO2. Nearly 100% coverage of perovskite film on sputtered TiO2 can be observed in the scanning electron microscopy images, obviously higher than 92% coverage on solution-based TiO2. The full coverage of perovskite and the proper band alignment between sputtered TiO2 and spiro-OMeTAD are two reasons responsible for the high open circuit voltage. The effects of annealing, growth temperature, sputtering target and thickness on performance of solar cell are also discussed. (C) 2016 Elsevier Ltd. All rights reserved.
更多
查看译文
关键词
Perovskite solar cell,Magnetron sputtering,Open circuit voltage,TiO2
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要