This research describes thiol-ene/epoxy hybrid networks for core-shell encapsulation of semiconductor devices. A thiol-ene network was formed using ultraviolet-induced radical polymerization, with unreacted thiols and epoxide monomers remaining in the network. Immersion in tributylamine catalyzed the thiol-epoxy coupling to produce a diffusion-limited hard outer shell. Tensile testing shows that the initial thiol-ene product (core) has elastomeric behavior, while the secondary curing creates a glassy material (shell) at room temperature due to thiol-epoxy coupling. Bulk samples of the material form a hard outer shell surrounding a soft core depending on the secondary cure conditions. There are positive relationships between wall thickness and secondary cure temperature and cure time, enabling control of shell thickness by varying reaction conditions. Shell thicknesses were measured up to 1.8 mm when immersed in tributylamine for up to 150 minutes and up to 140 °C. The ability to control core-shell thickness of dual-cured networks is applicable in device encapsulation processes. Core-shell encapsulants for microelectronics may provide further shock and impact protection for durable electronic devices. Further aging and operational studies will be needed to determine time-stability and optimal processing of the core-shell structure.
更多
查看译文
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要