Internal curing of high performance mortars with bottom ash

Mateusz Wyrzykowski,Sadegh Ghourchian,Sakprayut Sinthupinyo, Natechanok Chitvoranund, Tipwimol Chintana,Pietro Lura

Cement and Concrete Composites(2016)

引用 71|浏览4
暂无评分
摘要
In Thailand, approximately 9500 tons of bottom ash are produced annually by the boilers of the SCG Paper business within the SCG conglomerate. In an effort to find high-value uses of this industrial waste and to limit landfilling, the internal curing performance of different types of bottom ash, both from stoker and circulating fluidized bed boilers was studied by means of internal relative humidity and autogenous deformation measurements on high-performance mortars. In this application, the bottom ash particles are pre-saturated with water, which is released during cement hydration and contributes to reduce self-desiccation and shrinkage of the mortars.
更多
查看译文
关键词
High-performance concrete,Shrinkage,Autogenous deformation,Internal curing,Bottom ash,Pore structure
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要