Mechanical twinning in Ni-based single crystal superalloys during multiaxial creep at 1050 °C
Materials Science and Engineering: A(2018)
摘要
Multiaxial high-temperature creep tests have been performed at 1050 °C on a first-generation Ni-based single-crystal superalloy through the use of asymmetric notched specimens. Mechanical twins have been observed by EBSD and TEM analyses. A finite element simulation in a crystal plasticity framework has also been carried out to better understand the presence of mechanical twins at stress concentrators depending on stress triaxiality, plastic strain rate, and damage level.
更多查看译文
关键词
Nickel base single crystal superalloy,Mechanical twinning,Deformation mechanism,Creep,High temperature