Exploring the Limits of Cobalt Liner Thickness in Advanced Copper Interconnects

IEEE Electron Device Letters(2019)

引用 29|浏览89
暂无评分
摘要
We investigate the performance and reliability characteristics of Cu interconnects with Ta-based barrier layers and Co wetting layers at 7nm node dimensions with a focus on the impacts of reducing the Co thickness from 30Å down to 10Å. We demonstrate that while reducing Co liner thickness significantly reduces RC delay, there is a significant reduction in electromigration reliability below a thickness of 20Å if used in conjunction with a PVD (physical vapor deposition) TaN barrier. However, if the PVD treatment is followed by deposition of a thin ALD (atomic layer deposition) TaN, the Co layer thickness can be scaled down to 10Å without any penalty in either electromigration or time dependent dielectric breakdown (TDDB.) The combined PVD/ALD process with 10Å Co enables a 14% reduction in RC delay relative to our control split.
更多
查看译文
关键词
Resistance,Metallization,Electromigration,Capacitance,Reliability,Electrical resistance measurement,Dielectric breakdown
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要