Effect of Cooling Rate and Slag Modification on the Copper Matte in Smelting Slag

MINING METALLURGY & EXPLORATION(2020)

引用 7|浏览12
暂无评分
摘要
The amount of copper flash smelting slag has increased during the recent years along with an increasing slag-to-metal ratio. During slag tapping, some copper sulfide is mechanically entrained. As a result, it is necessary to recover copper matte from the slag by suitable methods. At present, the most common way is slow, controlled cooling in a transfer ladle. However, research on the detailed effects of slow cooling and the function of slag modification is rare. This paper described experiments that were performed at different cooling rates (0.5, 1.5, 3, and 7 °C/min), with and without additive. A detailed characterization of the copper-rich phase and its particle size was subsequently made using SEM-EDS micrographs and image analysis software. With a decrease in cooling rate, the particle size of the copper-rich matte phase became larger. The addition of gypsum and carbon as a slag modifier affected the size of the copper-rich phase slightly, and its chemical composition was modified compared with the experiments without additive.
更多
查看译文
关键词
Slag cleaning,Ladle cooling,Copper matte,Image analysis
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要