Thermal Stability Of Mgo Film On Si Grown By Atomic Layer Deposition Using Mg(Etcp)2 And H2o

CERAMICS INTERNATIONAL(2021)

引用 2|浏览3
暂无评分
摘要
MgO films were deposited on Si via atomic layer deposition (ALD) using Mg(EtCp)2 and H2O precursors and their thermal stability was examined as a function of the post-deposition annealing (PDA) temperature. The characteristic self-limiting behavior of the ALD process was confirmed by changing several parameters, such as precursor pulsing times, deposition temperature, and number of cycles. The exceptional resulting step coverage was verified on a patterned wafer with a high aspect ratio. The band gap and dielectric constant of the as-deposited ALD-MgO film were extracted to be approximately 7.5 eV and 8.4, respectively, and were stable up to the PDA temperature of 700 degrees C. However, considerable outward diffusion of the underlying Si atoms toward MgO started to occur above 700 degrees C, and most of the MgO film was converted to an amorphous Mg-silicate phase at 900 degrees C with a thin layer of remaining MgO on top.
更多
查看译文
关键词
MgO, Atomic layer deposition, Thermal stability, Interfacial reaction, Si out-diffusion
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要