Homogenization behavior of IN 718 superalloy prepared by electron beam layered solidification technology
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T(2021)
摘要
The homogenization behavior of IN 718 superalloy prepared by electron beam layered solidification has been investigated at 1150 degrees C. The set temperature was accurately corrected as 1149 degrees C by a compound method. The effect of homogenization treatment on the microstructure and microsegregation evolution was discussed by two models. A further discussion about Nb diffusion was conducted. The results show that the microsegregation was eliminated after the ingot was homogenized for 8 h at 1150 degrees C. Meanwhile, D-Nb and D-Ti is calculated approximately as 3.8 x 10(-11) cm(2)/s and 4.0 x 10(-11) cm(2)/s, respectively. The completion time of homogenization at a certain temperature depends on the degree of segregation, the distance between the secondary dendrite arms and the content of Nb. Additionally, it seems like that the D-Nb in IN 718 alloy decreases with the decrease of its concentration at the same temperature. (C) 2021 The Author(s). Published by Elsevier B.V.
更多查看译文
关键词
Homogenization behavior,Electron beam smelting,Layered solidification technology
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要