Experiments and crystal plasticity simulations for the deformation behavior of nanoindentation: Application to the 2 phase of TiAl alloy
Materials Science and Engineering: A(2022)
摘要
In this work, nanoindentation experiments were carried out to investigate the deformation behavior of alpha 2 phase in Ti-43.5Al-4Nb-1Mo-0.1B alloy. The crystal plasticity simulations of nanoindentation process were implemented using the crystal orientation information obtained from the EBSD results. Through the combination of crystal plasticity finite element simulations and nanoindentation experiments, the constitutive parameters were calibrated and verified by comparing the hardness of simulated and experimental results. The mean error between simulation and experiment was 7.89%, which confirmed the accuracy of parameter calibration. Besides, the surface topography and the slip behavior were analyzed by the calculation of Schmid factors. Results revealed that the slip and pileup tend to occur at the areas with a large surface Schmid factor (SSF) and a small interior Schmid factor (ISF). In addition, the hardness and its connection with the slip behavior were discussed. It was found that the hardness of each grain is closely related to its crystal orientation. Among all the tested grains, the grain with Euler angle of (115.5 degrees, 80.1 degrees, 8.4 degrees) has the lowest value of hardness, and the slip system (1100) [1120] plays a leading role in the deformation at the center of indentations.
更多查看译文
关键词
Nanoindentation,Crystal plasticity simulation,Pileup,Schmid factors,Slip behavior,Hardness
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要