Quantitative Analysis of Nickel-Based Superalloys Based on a Remote LIBS System
Spectroscopy and Spectral Analysis(2022)
摘要
Based on the self-designed remote laser-induced breakdown spectroscopy (LIBS) system, the focusing characteristics of remote LIBS were analyzed, and the experimental method of quantitative analysis of nickel-base superalloy by remote LIBS was studied. In this LIBS system, the laser focusing and the plasma optical signal acquisition optical paths are coaxial and independently focused. Through automatic focusing, the remote analysis of 1 similar to 10 m can be achieved. The results show that affected by the depth of focus, the detectable range of plasma optical signal increases with the increase of working distance. That is, the requirement of the LIBS system for focusing accuracy decreases. At the same time, the decrease of power density caused by the increase of ablation spot size and the decrease of signal acquisition solid angle make the spectral line intensity attenuate in inverse proportion to the fourth power as the working distance increases. In this paper, the standard curves of Ni, Cr, Nb, Mo, Ti and Al in GH4169 nickel-based superalloy were established using the standard curve method without internal standard with internal standard. The goodness of fit of the standard curve with internal standard (0. 999 7, 0. 999 4, 0. 999 87, 0. 999 1, 0. 998 1 and 0. 999 7) was significantly better than that of the standard curve without internal standard (0. 953 2, 0. 876 6, 0. 897 4, 0. 914 5, 0. 938 4 and 0. 991 6). Finally, LIBS and XRF were compared. For major elements Ni, Cr, Nb and Mo, the relative standard deviations of the two methods were 1. 75%similar to 3. 90% and 0. 10%similar to 0. 52% , and the relative errors were 0. 48% similar to 0. 92% and 0. 64%similar to 2. 25% , respectively; for trace elements Ti and al, the relative standard deviations of the two methods were 5. 58% , 5. 86% and 2. 39% , 5. 64% , the relative error is 2. 75% , 3. 14% and 4. 68% , 2. 39% respectively. Due to the instability of plasma, the precision of the remote LIBS method is slightly lower than that of the XRF method. However, LIBS method can effectively reduce the measurement error through repeated measurements, which indicates that LIBS technology is feasible for remote on-line analysis of nickel-based superalloys.
更多查看译文
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要