The Spread of Corrosion of the Deposited Material Using the Cold Spray Method

ECS Transactions(2021)

引用 0|浏览0
暂无评分
摘要
A layer of copper was applied to the base aluminum material using the cold spray method (cold kinetic deposition). The samples were exposed to corrosion in a salt chamber for 100, 200 and 300 hours. The change in the size of the internal and surface resistance of the samples was monitored. The corrosion results were also examined using an electron microscope.