Capacity fade detection in lithium-ion batteries using non-linear frequency response analysis (NFRA) under multiple open-circuit voltages (OCVs)
Electrochemistry Communications(2022)
摘要
•Capacity loss detection using Total harmonic distortion under multiple SOCs.•Applicability of Nonlinear frequency analysis on commercial lithium-ion cells.•Harmonic distortions are dependent on SOC below 1 Hz.•Aging quantification for all SOCs under the range of 10 Hz–150 Hz.•Different harmonic responses for the cells aged at different temperatures.
更多查看译文
关键词
Lithium-ion battery,Nonlinear frequency response analysis,State of health,Harmonic distortions