Formation and annihilation of deformation twinning in hexagonal Ti with lamellar microstructure

Journal of Alloys and Compounds(2022)

引用 3|浏览2
暂无评分
摘要
The microstructural evolution and mechanical properties of Ti35 alloy applied in nuclear industry with lamellar microstructure during high-temperature straining were systematically investigated. Ti35 alloy plates were subjected to hot rolling down to 20 %, 50 % and 80 % reduction in thickness. Results showed that {101̅2}<101̅1̅>, {112̅2}<112̅3̅>and {101̅1}<101̅2̅>twins were developed during hot rolling and their proportion varied with the amount of deformation. The fraction of twinning boundary reached peak value in the 50 % reduction sample, which dominated by {101̅2}<101̅1̅>and {112̅2}<112̅3̅>twins. After annealing, the deformation twins in>50 % reduction samples were nearly annihilated. The twins and substructures acted as nucleation point for static recrystallization, resulting in twins annihilated and grain refinement during annealing. Micro-hardness and tensile tests revealed that deformation twinning improved strength and plasticity of the Ti35 alloy by introducing extra interfaces and reorientation.
更多
查看译文
关键词
Ti35 alloy,α lamellar,Deformation twinning,Twins annihilation,Dynamic recovery
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要