This work aims to investigate the processability of Rene 80 via laser powder-bed fusion (L-PBF). Rene 80 is a poorly weldable Ni-superalloy, currently processed via investment casting to fabricate turbine blades working at an operating temperature of about 850 degrees C. The L-PBF parameters optimization aims to increase part integrity and enhance processing repeatability. This part was tackled by creating a complete design of experiments (DOE) in which laser power, scan speed and hatching distance were varied accordingly. Optimizing the abovementioned parameters minimized the crack density and pore area fraction. Hence, five parameter sets leading to a crack density lower than 100 mu m/mm(2) and a pore fraction between 0.045% and 0.085% were selected. Furthermore, the intra-print repeatability was studied by producing three specimens' repetitions for each optimal set of parameters in the same build. The porosity value obtained was constant among repetitions, and the crack density (around 75 mu m/mm(2)) had a slight standard deviation. The third step of the research assessed the inter-prints repeatability by producing a replica of the five selected parameter sets in a different build and by comparing the results with those studied previously. According to this latter study, the porosity fraction (ca. 0.06%) was constant in intra- and inter-print conditions. Conversely, crack density was lower than 100 mu m/mm(2) only in three sets of parameters, regardless of the intra- or inter-build cross-check. Finally, the best parameter set was chosen, emphasizing the average flaw fraction (least possible value) and repeatability. Once the optimal densification of the samples was achieved, the alloy's microstructural features were also investigated.
更多
查看译文
关键词
laser powder bed fusion,nickel-based superalloys,parameter optimization,repeatability
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要