Foaming during vitrification of radioactive waste in Joule-Heated Ceramic Melters (JHCM) is exacerbated by trapping of evolving gases, such as CO2, NOx and O2, beneath a viscous reaction layer. Foaming restricts heat transfer during melting. Sucrose is employed as the baseline additive at the Hanford site in Washington State, USA to reduce foaming. Alternative carbon-based reductant additives were explored in simulated, inactive Hanford high-iron HLW-NG-Fe2 feeds, for both their effect on foaming and to give insight to the behaviour of multivalent species in glass melts under different redox conditions. Graphite, coke (93% C), formic acid and HEDTA additives were compared with sucrose, and a feed with no additive. Graphite and coke additions proved most effective in reducing the maximum foam volume by 51 +/- 3% and 54 +/- 2%, respectively, compared with 24 +/- 5% for sucrose. Lower foaming could result in more efficient vitrification in JHCMs. Reductants also affected redox ratios in the multivalent species present in the feed. The order of reduction, Mn3+/Mn2+ > Cr6+/Cr3+ > Ce3+/Ce4+ > Fe3+/Fe2+ was as predicted on the basis of their redox potentials. There is less reduction overall, particularly in the Fe3+ -> Fe2+, than predicted by the calculations, attributed to the oxygenated atmosphere of the experiments.
更多
查看译文
关键词
high-iron level waste,foam control,alternative reductants,vitrification
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要