Stable chemical enhancement of passivating nanolayer structures grown by atomic layer deposition on silicon.
Nanoscale(2023)
摘要
Incorporation of carrier-selective passivating contacts is on the critical path for approaching the theoretical power conversion efficiency limit in silicon solar cells. We have used plasma-enhanced atomic layer deposition (ALD) to create ultra-thin films at the single nanometre-scale which can be subsequently chemically enhanced to have properties suitable for high-performance contacts. Negatively charged 1 nm thick HfO films exhibit very promising passivation properties - exceeding those of SiO and AlO at an equivalent thickness - providing a surface recombination velocity (SRV) of 19 cm s on -type silicon. Applying an AlO capping layer to form Si/HfO/AlO stacks gives additional passivation, resulting in an SRV of 3.5 cm s. Passivation quality can be further improved simple immersion in hydrofluoric acid, which results in SRVs < 2 cm s that are stable over time (tested for ∼50 days). Based on corona charging analysis, Kelvin probe measurements and X-ray photoelectron spectroscopy, the chemically induced enhancement is consistent with changes at the dielectric surface and not the Si/dielectric interface, with fluorination of the AlO and underlying HfO films occurring after just 5 s HF immersion. Our results show that passivation is enhanced when the oxides are fluorinated. The AlO top layer of the stack can be thinned down by etching, offering a new route for fabrication of ultra-thin highly passivating HfO-containing nanoscale thin films.
更多查看译文
关键词
atomic nanolayer deposition,nanolayer structures,silicon,stable chemical enhancement
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要