Anisotropic Creep Behavior of DD15 Single Crystal Superalloy
RARE METAL MATERIALS AND ENGINEERING(2022)
摘要
DD15 single crystal superalloy with [001], [011] and [111] orientations was cast by seed method in the directional solidified furnace. The creep properties of the alloy with different orientations were investigated at 980 degrees C/300 MPa. In order to obtain the microstructure evolution after different creep time, the creep after 50 and 100 h and the creep fracture of three kinds of tests were investigated. The alloy microstructure with different orientations were investigated by SEM and TEM. The results show that the alloy with different orientations has obviously various microstructure characteristics on the section perpendicular to the crystal growth direction. The gamma' phase with [001] orientation is regular square, that with [011] orientation is rectangular, and that with [111] orientation is polygon. The creep properties of the alloy exhibit obvious anisotropy at 980 degrees C/300 MPa. The creep life of the alloy decreases in the sequence of [111], [001] and [011] orientation. The creep strain of the alloy under different conditions decreases in the sequence of [001], [011] and [111] orientation. The common feature of the creep curves is a very short primary creep stage. Compared with creep curves of the [001] and [111] orientation, the creep curve of [011] orientation has a shorter third creep stage. The degree of gamma' coarsening is obviously different for alloy with different orientations after creep. The rafting speed of [001] oriented sample is larger than that of [011] and [111] oriented sample. After creep fracture, the dislocation network of [001] or [111] oriented alloy is denser and better than that of [011] oriented alloy.
更多查看译文
关键词
single crystal superalloy, DD15, creep behavior, anisotropy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要