Cognition on Oxidation Behavior of Ni-based Superalloy GH4742 when Exposed to Water Vapor
Journal of Materials Science and Technology/Journal of materials science & technology(2024)
摘要
The oxidation behavior of Ni-based superalloy GH4742 exposed to water vapor was investigated at 900- 1100 & DEG;C for 50 h in Ar + 20%H2O, with Ar + 20%O 2 included for comparison. The presence of H2O is adverse to formation of continuous Cr2O3 oxide layer but contributes to generation of big voids. Based on this, Ni2+ and Co2+ are more easily to diffuse towards the outermost oxide layer (OOL), forming non-protective Ni-and Co-rich oxides with high proportion. This leads to a higher weight gain in Ar + 20%H2O than that in Ar + 20%O 2 . At elevated temperatures, the spallation of oxide scale occurs while the consumption of Cr is reduced in Ar + 20%H2O, and the contents of Ni-and Co-rich oxides at this moment are reduced in the OOL. The oxidation mechanism was also discussed.& COPY; 2023 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
更多查看译文
关键词
GH4742,Superalloy,H 2 O,Diffusion,Oxidation,Mechanism
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要