Area-Selective Atomic Layer Deposition of ZnO on Si\SiO2 Modified with Tris(dimethylamino)methylsilane
MATERIALS(2023)
摘要
Delayed atomic layer deposition (ALD) of ZnO, i.e., area selective (AS)-ALD, was successfully achieved on silicon wafers (Si\SiO2) terminated with tris(dimethylamino)methylsilane (TDMAMS). This resist molecule was deposited in a home-built, near-atmospheric pressure, flow-through, gas-phase reactor. TDMAMS had previously been shown to react with Si\SiO2 in a single cycle/reaction and to drastically reduce the number of silanols that remain at the surface. ZnO was deposited in a commercial ALD system using dimethylzinc (DMZ) as the zinc precursor and H2O as the coreactant. Deposition of TDMAMS was confirmed by spectroscopic ellipsometry (SE), X-ray photoelectron spectroscopy (XPS), and wetting. ALD of ZnO, including its selectivity on TDMAMS-terminated Si\SiO2 (Si\SiO2\TDMAMS), was confirmed by in situ multi-wavelength ellipsometry, ex situ SE, XPS, and/or high-sensitivity/low-energy ion scattering (HS-LEIS). The thermal stability of the TDMAMS resist layer, which is an important parameter for AS-ALD, was investigated by heating Si\SiO2\TDMAMS in air and nitrogen at 330 & DEG;C. ALD of ZnO takes place more readily on Si\SiO2\TDMAMS heated in the air than in N-2, suggesting greater damage to the surface heated in the air. To better understand the in situ ALD of ZnO on Si\SiO2\TDMAMS and modified (thermally stressed) forms of it, the ellipsometry results were plotted as the normalized growth per cycle. Even one short pulse of TDMAMS effectively passivates Si\SiO2. TDMAMS can be a useful, small-molecule inhibitor of ALD of ZnO on Si\SiO2 surfaces.
更多查看译文
关键词
area selective, atomic layer deposition, silane, silicon, inhibitor, ZnO
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要