Archeological wood conservation with selected organosilicon compounds studied by XFM and nanoindentation
Wood Science and Technology(2023)
摘要
Waterlogged wood conservation is a complex and challenging task. Detailed knowledge about the interactions between the applied chemicals and wood is necessary to ensure the effective and safe conservation of wooden artifacts. The present research aims to determine the mechanism of dimensional stabilization of archeological wood by organosilicon compounds using the combination of synchrotron-based X-ray fluorescence microscopy (XFM) and nanoindentation. Archeological oak wood was treated with methyltrimethoxysilane, (3-mercaptopropyl)trimethoxysilane, or 1,3-bis-[(diethylamino)-3-(propoxy)propan-2-ol]-1,1,3,3-tetramethyldisiloxane, which in previous studies were found to be more effective than other organosilicons in stabilizing wood dimensions. The XFM and nanoindentation results showed that all three organosilicons infiltrated wood cell walls and enhanced their mechanical properties. The XFM also showed that part of the chemicals filled some void spaces like cell lumina. Based on the results obtained here and in our previous research, it is determined that the mechanism of archeological wood dimensional stabilization by organosilicon treatment is complex and likely involves both filling cell lumina and infiltration into cell walls where organosilicons interact with wood polymers.
更多查看译文
关键词
archeological wood conservation,organosilicon compounds
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要