Application of Machine Learning in Automotive Stud Weld Defect Classification

IEEE Sensors Journal(2023)

引用 0|浏览1
暂无评分
摘要
Arc stud welding (ASW) is a well-developed and automated manufacturing process commonly used to fasten studs to a workpiece. This process requires the implementation of measures to prevent low-quality welds that can lead to the disposal of an entire structure. In this article, a machine learning-based method is introduced that uses experimental data to detect and classify defective stud welds. The source of data is a series of experimental arc stud welds conducted by a precision robotic arm. Welding data log is recorded through various sensors to shape a multivariate dataset for ASW. Then, wavelet transforms (WTs) as well as synthetic signal generation are applied for feature extraction. For each set of extracted features, suitable models are designed, trained, and evaluated for automatic root cause classification. Next, the models and approaches are compared on synthetic measurement generation, feature extractions, and feature importance. Numerical results show that XGBoost, the best model, has an 85.41% F1-score on the test set. Additionally, the study reveals that voltage and lift play crucial roles in the root cause classification of arc stud weld. The proposed method not only offers promising results for defect detection in ASW but also provides outreach value for similar industrial processes.
更多
查看译文
关键词
machine learning,classification
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要