Effect of Ca addition on microstructure and mechanical properties of Mg-3.8Al-1.1Sn alloys

MATERIALS TODAY COMMUNICATIONS(2024)

引用 0|浏览3
暂无评分
摘要
Achieving high strength and high ductility simultaneously is challenging, limiting the industrial application of Mg alloys. However, effective approaches such as grain refinement and texture weakening have emerged to address this challenge. Herein, we design a novel processing strategy incorporating the addition of Ca to Mg-AlSn alloys and asymmetric severe shear extrusion (ASSE). This strategy aims to refine the grain structure and promote the formation of dispersed nano -sized CaMgSn phases. The extruded Mg-3.8Al-1.1Sn-0.4Ca sheets exhibit a yield strength (YS) of -220 MPa, an ultimate tensile strength (UTS) of -320 MPa, and an elongation (EL) of -18.0%, which achieving a good combination of strength and ductility through a single -pass extrusion.
更多
查看译文
关键词
Mg-Al-Sn,Ca addition,Sub -rapid solidification,Asymmetric severe shear extrusion
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要