316L stainless steel is widely used in various industrial fields, but its strength is relatively low. The improvement of its strength has become a research hotspot. In this study, nano titanium carbide (TiC) particles are ball milled with 316L with the addition of 2 wt% and 4 wt%. The composite powder was then used for the fabrication of samples by laser powder bed fusion. The results show that the TiC is uniformly distributed in the microstructure. With the addition of TiC, the average size of the grains is significantly reduced. The strength, hardness, and wear resistance of TiC/316L samples have been greatly improved. The tensile strength of formed 2 wt% TiC/316L is 948 MPa, together with a extension rate of 36.0%, which has been increased by 42.6% and 79.7%, respectively. This study provides an effective way to improve the strength at room temperature and the high temperature of 316L built by laser powder bed fusion.
更多
查看译文
关键词
316L,laser powder bed fusion,TiC,mechanical property,high temperature property
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要