In this paper, the effects of Hafnium (Hf) doping on the crystal structures and piezoelectric properties of aluminum nitride (AlN) thin films were reported. Aluminum nitride based (HfxAl1-xN) films with different Hf concentrations were deposited on Si (100) substrates by adjusting the RF power to vary the dopant concentration. The optimum doping ratio and process parameters for optimizing the piezoelectric properties of the proposed films were investigated using various material analysis techniques such as X-ray Photoelectron Spectroscopy (XPS), X-ray diffractometer (XRD), Atomic Force Microscope (AFM), and Piezoresponse Force Microscopy (PFM). The results showed that the best properties of the proposed films were obtained with 12.1 at % Hf doping, and the c/a ratio of the material was 1.561, which confirmed the lattice structure transformation from wurtzite to hexagonal structure. The piezoelectric coefficient d33 was 10.34 p.m./V, 220 % higher than the undoped AlN film. The film bulk acoustic resonators (FBARs) using the proposed film were then fabricated. It was found that the electro-mechanical coupling coefficient (K2eff) was increased to 10.43 % using 12.1 at% Hf-doped AlN piezoelectric film, which is an abrupt increase of the undoped AlN FBAR (with an electro-mechanical coupling coefficient of 7.1 %). It demonstrates the significant potential of using proposed films for broadband applications.
A single-structure three-axis MEMS accelerometer often suffers from cross-axis interference, which leads to inaccurate sensitivity and makes it difficult to reliably assess the health condition of the measured object. In addition, achieving high sensitivity often comes at the cost of reduced bandwidth. Because few previous studies have addressed the cross-axis interference of such structures, this study presents the development and optimization of a structural three-axis MEMS piezoelectric accelerometer. A mathematical model was first established, followed by simulation and structural optimization to enhance sensitivity and minimize cross-axis interference while keeping the bandwidth nearly unchanged. This study proposes, for the first time, an improved structure that evolves the L-shaped accelerometer into a composite configuration consisting of a W-shaped cantilever and an additional four-bar proof mass, in order to enhance bandwidth and significantly reduce cross-axis interference. Generally, an increase in sensitivity leads to a reduction in bandwidth; however, by modifying the geometry of the proof mass, the proposed accelerometer achieves a substantial improvement in sensitivity while avoiding a significant loss of bandwidth. The implementation of a triaxial accelerometer can generally be achieved in three ways: using three single-axis accelerometers, realizing three axes through circuitry, or achieving three axes through structural design. Using three single-axis accelerometers results in large volume, heavy weight, and high cost. Circuit-based three-axis implementation cannot detect multi-axis forces simultaneously, whereas structural three-axis design is difficult to realize. This study focuses on designing a triaxial accelerometer based on a structural approach, optimizing it with reference to the most successful examples reported in the literature and progressively addressing the drawbacks of previous structures. First, trapezoidal beams are used instead of rectangular cantilever beams to increase bandwidth. Next, two additional cantilever beams are added to transfer the Z-axis sensitivity detection points to reduce cross-axis interference. Finally, the shape of the proof mass is designed to enhance the sensitivities along all three axes. The optimized accelerometer exhibits resonant frequencies of approximately 12.6 kHz, 31.6 kHz, and 11.8 kHz along the X-, Y-, and Z-axes, with corresponding sensitivities of 6.11, 5.44, and 8.85 mV/g, and cross-axis interference reduced to below 15%. The results demonstrate the achievement of a highly accurate and reliable three-axis MEMS piezoelectric accelerometer through structural design and optimization. The proposed design concept may also be beneficial for other piezoelectric-based sensor applications.
In this study, the microstructure, electrical properties of the lead-free (Na0.52K0.4425Li0.0375)(Nb0.8925Sb0.07Ta0.0375)O-3 (NKLNTS) + 2.0 mol% MnCO3 + y mol% LiF (y = 0 similar to 3.0) ceramics sintered in air and reduced atmosphere are investigated. Both the density and grain size increase as y = 1. The samples sintered in air showed Delta T = 1.02 K of 30 kV/cm at 313 K. This is because introducing low radius Li+ ions forms an A-site substituted cell structure and changes the internal lattice stress, thus improving the polarization and electrocaloric performance. In contrast, sintered in a reduced atmosphere shows a negative effect of -0.812 K due to the enhanced polarization of defect dipoles, offsetting the decrease in maximum polarization, causing the maximum polarization to increase with increasing temperature. In addition, the observation of defect relaxation phenomena contributes to a wider operating temperature range. This is an important step towards refrigerating ferroelectric ceramics sintered in a reduced atmosphere.
In this work, lead-free (Na0.475K0.475Li0.05)NbO3 + x wt.% ZnO (NKLN, x = 0 to 0.3) piezoelectric ceramics with high piezoelectric g-coefficients were prepared by conventional solid-state synthesis method. By adding different concentrations of ZnO dopants, we aimed to improve the material properties and enhance their piezoelectric properties. The effects of the ZnO addition on the microstructure, dielectric, piezoelectric and ferroelectric properties of the proposed samples are investigated. Adding ZnO reduced the dielectric constant and improved the g-value of the samples. The properties of the samples without ZnO doping were g33 = 31 mV·m/N, g15 = 34 mV·m/N, kp = 0.39, Qm = 92, εr = 458, d33 = 127 pC/N and dielectric loss = 3.4%. With the preferable ZnO doping of 1 wt.%, the piezoelectric properties improved to g33 = 40 mV·m/N, g15 = 44 mV·m/N, kp = 0.44, Qm = 89, εr = 406, d33 = 139 pC/N and dielectric loss = 2.4%. Finally, ring-shaped shear mode piezoelectric accelerometers were fabricated using the optimum ZnO-doped samples. The simulated resonant frequency using ANSYS 2024 R1 software was approximately 23 kHz, while the actual measured resonant frequency of the devices was 19 kHz. The sensitivity was approximately 7.08 mV/g. This piezoelectric accelerometer suits applications requiring lower sensitivity and higher resonant frequencies, such as monitoring high-frequency vibrations in high-speed machinery, robotic arms or scientific research and engineering fields involving high-frequency vibration testing.
In this study, we utilized the tape-casting method to produce Pb-free (Na0 & sdot;52K0 & sdot;4425Li0.0375) (Nb0 & sdot;8925Sb0 & sdot;07Ta0.0375)O3 + 2 mol% MnCO3 + y mol% LiF (y = 0 to 3) piezoelectric ceramics. We investigated the impact of LiF sintering in a reduced atmosphere on microstructure, dielectric properties, impedance spectroscopy, and piezoelectric performance. By analyzing the degree of diffuse phase transition, we observed increased density and enhanced long-range order in the sample doped with 1 mol% LiF, which exhibited optimal piezoelectric properties (d33 = 265 pC/N and kp = 0.437) and a minimal diffusion parameter. Moreover, LiF doping enabled sintering at 1020 degrees C under low PO2, facilitating potential co-firing with Cu inner electrodes to further enhance the piezoelectric performance. Using the optimized parameters, we fabricated a cross-type triaxial piezoelectric accelerometer, demonstrating sensitivities of 2.33, 2.44, and 10.6 mV/g along the X, Y, and Z axes, respectively, with a resonance frequency of -2600 Hz and frequency range of -1300 Hz. This accelerometer holds promise for vibration measurements in low-frequency mechanical systems.