The fast-growing display industry demands coatings on increasingly large glass substrates. Conventional vertical magnetron sputtering requires a substrate carrier, which raises equipment cost and wastes material in carrier-covered regions. A carrier-free inclined-substrate configuration (85° inclination), therefore, offers higher material utilization and lower cost. This work presents the magnetic-circuit design and field-uniformity optimization of a large-area rectangular magnetron sputtering target for such substrates. The magnetic flux density between the target and the substrate is obtained from an analytical magnetic-charge integration model and compared with 3D magnetostatic COMSOL simulations using the “Magnetic Fields, No Currents” interface for N42 NdFeB magnets (1.3 T remanence). The straight section is optimized parametrically through flux-concentrating/guiding structures and magnet dimensions, and the end region is evaluated across four configurations. The adopted end design (a semicircular inner strip plus a semitoroidal outer ring) reduces the maximum curve separation Sm—the maximum lateral distance between the end-region and straight-section field curves—from 143 to 12.5 mm (a 91.3% reduction), while the peak horizontal flux density, measured at the cathode-sheath height along the erosion-zone centerline, changes from 58.3 to 54.7 mT. The 54.7 mT peak lies marginally above the 30–50 mT engineering target range and should be brought back into the interval in a subsequent refinement. This is a computational study; the predicted fields and the anticipated process benefits require experimental validation.
We report the adverse impact of Mg diffusion from a heavily doped p++ GaN cap layer on the optically active acceptor density and radiative recombination performance of the underlying p-GaN layer grown by metalorganic chemical vapor deposition. Secondary ion mass spectrometry depth profiling confirms significant longitudinal Mg diffusion from the p++ cap layer into p-GaN, leading to a total Mg concentration comparable to that of directly in situ doped samples. However, 30 K low-temperature photoluminescence measurements reveal that this diffusion-induced Mg increment hardly contributes to the density of optically active MgGa acceptors and instead introduces massive defect centers that suppress radiative recombination in p-GaN. The performance degradation is attributed to interstitial Mg and charged defect complexes introduced by diffusion, which induce strong ionized impurity scattering and reduce the radiative recombination probability of photogenerated carriers. This finding provides critical guidance for the p-type doping structure design of GaN-based optoelectronic and power electronic devices.
Neutral-beam and neutral-beam-assisted reactive etching circumvent the plasma-process-induced damage, which originates from surface charging and ultraviolet radiation. For high-aspect-ratio etching, a tightly collimated beam is needed to avoid sidewall distortion and subsurface modifications of the atomic structure; e.g., for an aspect ratio of 100, scattering must be kept small beyond a divergence angle of θtol ≈ 0.01 rad and set to 0.25° (lab frame) in this study. The directionality of the beam will depend on several design factors. In this work, we examine a gas-phase neutral beam source based on charge-exchange conversion of energetic ions, focusing on the fundamental constraints imposed by ion–atom and atom–atom scattering in the neutralization region. For argon ions and fast neutrals in the keV range, scattering at angles θ > θtol is dominated by the repulsive wall of the interaction potential, which is well described by a Born–Mayer form Ae−br. This yields a simple yet accurate model suitable for Monte Carlo simulations. In particular, a known method is used to compute the scattering angle, θ(p), where p is the impact parameter. The angle is given in terms of a modified Bessel function, whose argument is obtained by solving a nonlinear equation. The model can be trusted to predict the angular distribution for θ > θtol and thus determine the flux scattered into these angles. We provide model-based predictions for the angular distributions, compare these with a representative experimental dataset, and propose a lumped one-dimensional formulation to describe both small- and large-angle scattered ion and fast-atom fluxes. The flux of fast atoms scattered at small angles θ < θtol, normalized to the incident ion flux, attains its maximum when L/λcx ∼ 1, where L is the beam propagation length and λcx is the mean free path for charge exchange.
SACLA is a Japanese x-ray free-electron laser (XFEL) facility that has been operating for academic and industrial users. A pulsed high-voltage electron gun equipped with a thermionic cathode made of a single-crystal CeB6 has been used to deliver high-brightness electron beams required for XFEL operation. Recently, an upgrade plan for SACLA based on electron-source technologies was proposed. This plan emphasizes not only upgrading the repetition rate but also improving XFEL light quality. The strategy and progress toward developing an ultimate thermionic electron gun for the SACLA upgrade are described in this paper.
Tetrahedral amorphous carbon (ta-C) films are promising protective materials, but their practical applications in harsh environments (high temperature, high mechanical load, and marine corrosion-wear conditions) are limited by high residual stress, poor adhesion, and insufficient stability. This study systematically investigates the effects of Cr doping (0–41.1 at. %) on the microstructure, mechanical, tribological, and corrosion properties of ta-C films prepared via a hybrid filtered cathodic vacuum arc and pulsed DC magnetron sputtering system. The core novelty lies in revealing Cr's dual regulatory mechanism: Cr doping promotes film graphitization (reducing residual stress) while inducing the formation of CrC hard nanophases (recovering mechanical properties), achieving synchronous stress reduction and performance enhancement. Specifically, low Cr content forms solid solutions in the carbon network, while excess Cr precipitates as face-centered cubic CrC; bond conversion from sp3 to sp2 accompanies graphitization, with hardness initially decreasing then increasing due to nanocomposite structure formation. The optimized Cr doping (9.6 at. %) realizes synergistic improvements in room-temperature/high-temperature (400 °C) dry tribological properties, simulated seawater tribological performance, and corrosion resistance (higher corrosion potential and lower corrosion current density). This work provides a new design strategy for balancing ta-C films’ comprehensive properties, offering experimental/theoretical support for their applications in marine engineering (ship propellers and seawater valves), high-temperature mechanical components (engine piston rings and aviation bearings), and other harsh-environment fields.