Conventional yarn abrasion testing determines the number of abrasion cycles to break but does not reveal the changes in yarn geometry that occur before failure. The aim of this study was to apply and evaluate a longitudinal image-based method for monitoring changes in yarn-body diameter during progressive abrasion. Eight yarns differing in linear density and construction were investigated in untreated, conventionally sized, and pre-wetted sizing conditions. Abrasion resistance was determined using a Zweigle G551 abrasion tester, with 20 specimens tested per yarn–treatment combination. Five of these specimens were monitored longitudinally by digital microscopy at predefined abrasion intervals until breakage or the final observation. Yarn diameter was determined using Fiji (ImageJ) and the Ridge Detection plugin. A supplementary methodological evaluation showed maximum deviations of 0.40–1.22% in a parameter-sensitivity assessment and differences of −1.35% to +2.50% between automated and manual measurements on representative images. Conventional sizing yielded the highest geometric mean cycles to break for all eight yarns, although statistically significant treatment effects were detected for six yarns. Longitudinal diameter changes varied among specimens and abrasion stages, with some yarns showing an initial decrease followed by stabilization or an increase. The results demonstrate the potential of repeated image-based measurements to complement conventional abrasion testing by characterizing changes in yarn geometry before failure. Further validation of image registration and measurement repeatability is required.
Undershirts are worn under athletic apparel in hot environments, but their effects on the skin-clothing microclimate and thermoregulation remain unclear. We investigated whether undershirt use and breathability affect intra-clothing environments and thermoregulatory responses during exercise. Thirteen male runners completed two 30 min treadmill bouts at moderate and high intensities, separated by a 10 min break (32 °C, 50% relative humidity, and 0.8 m/s). They wore a polyester T-shirt with a regular polyester undershirt (CON), an undershirt with greater air permeability under wet conditions (Dry Aeroflow, DAF), or no undershirt (NU) in a randomized crossover manner. Compared with NU, wearing undershirts increased chest intra-clothing humidity by up to 7% (all p ≤ 0.005). Overall, back sweat rate, wear discomfort, and trunk skin temperatures were ~0.1 mg/cm2/min, ~0.5, and ~0.5 °C higher, respectively, in CON and DAF than in NU (all p ≤ 0.043). Compared with CON, DAF reduced back sweat rate by ~0.06 mg/cm2/min and back intra-clothing temperature by ~0.22 °C (both p ≤ 0.014). No significant differences were detected in rectal temperature, mean skin temperature, heart rate, or body mass loss (all p ≥ 0.067). Collectively, undershirts altered local intra-clothing environments and physiological/perceptual responses, whereas DAF partially alleviated these local responses without altering whole-body physiological responses.
When glass filaments are bundled as a yarn and impregnated with a polymer, the analysis of the strength distribution becomes complex, as filament load-sharing and coating efficiency govern rupture, especially under alkali attack. This study investigates the tensile strength and its statistical characteristics of acrylic-impregnated E-glass yarns, containing 4200 filaments of 17 μm in diameter and a polymer content of 17%, before and after alkaline exposure, along with the corresponding uncoated yarn. The tensile strength of the uncoated yarn is found to be lower than that estimated for a single filament, with a gradual reduction in stiffness due to progressive filament failure originating at 40% of the yarn strength. Both the uncoated and impregnated yarns exhibited Weibull strength distributions, with the latter having a substantially higher Weibull modulus. Importantly, the coating leads to yarn strength much beyond that of the greige and about 10% higher than the estimated single filament strength while maintaining the stiffness up to failure, indicating that the polymer matrix governs filament load-sharing and failure. This could be attributed to the higher Weibull modulus of the impregnated yarn (i.e., 18 for coated yarn versus 9 and 7 for the greige and single filament, respectively). The impregnated yarns were also tested after exposure to an alkaline solution with pH 13 for 7, 28, and 56 days. Such attack caused only marginal strength loss after 7 days but later reduced the mean yarn strength by 33% after 56 days. Despite such degradation, the elastic modulus, coefficient of variation of the strength, and Weibull modulus remained unchanged throughout the exposure period. The results suggest that alkaline exposure predominantly leads to propagation of existing flaws rather than introducing new, larger defects. The findings through the Weibull analysis demonstrate that polymer-impregnation of E-glass yarn increases strength, lowers variability and promotes stiffness retention until rupture. Moreover, alkaline degradation shifts the strength distribution toward lower values without substantially increasing its scatter.
Aramid fibers combine high specific strength, impact-energy absorption and thermal stability, yet the same rigid, highly oriented chains also produce a chemically inert surface, low compressive strength and sensitivity to ultraviolet (UV) radiation and hydrolysis. This review synthesizes original research articles, indexed in the Web of Science Core Collection, with emphasis on 2021–2026, on how fiber- and fabric-level functionalization affects the structural and functional integrity of aramid composites. Unlike previous reviews, organized by method, material form or application, it follows the retention of this integrity from fiber to component. Plasma, chemical, bio-inspired and nano structural treatments are compared by interfacial gain, fiber damage and property retention after UV exposure. The roles of aramid nanofibers, matrices, processing, hybridization and shear-thickening fluids are discussed, together with added functions such as electromagnetic shielding, strain sensing, thermal management, liquid repellence and self-healing. Several interphases, including oxide layers and aramid nanofiber coatings carrying conductive phases, strengthen adhesion while protecting the fiber or adding a function, but most data refer to unaged fibers or small specimens tested for one property at a time. An evaluation framework is proposed that links fiber, laminate and component scales with combined aging, icing and electromagnetic requirements for outdoor structures.
Fluorescence is a powerful tool to realize textile products with high-visibility effects. Fluorescent materials can transfer non-visible UV light into visible light, and by doing so, the visibility under illumination with sunlight increases. For textile products, the application of fluorescence dyes on synthetic fibers is broadly used. However, fluorescence applications are rarely reported for regenerated cellulosic fibers, such as lyocell. For this, the actual study reports on a selection of five different fluorescence dyes investigated for applications in cotton and lyocell fabrics. Dyes are considered acid dyes, basic dyes and reactive dyes, and dye application is done in increasing concentrations. Prepared textile samples are investigated according to color strength and color shade (K/S values and CIE Lab coordinates). Fluorescence emission is determined by fluorescence spectroscopy. Fastness properties are measured against rubbing, washing and light. The attained coloration increases with increased applied dye concentrations. In contrast, the achieved fluorescence emission differs strongly depending on the dye, and also, for some dye/fiber combinations with low applied dye concentration, a higher fluorescence emission is achieved. For most investigated samples, superior fluorescence effects are gained for applications in lyocell compared to simultaneously treated cotton fabrics. Especially for the investigated reactive fluorescence dyes, excellent fastness properties against rubbing, washing and light are observed. Finally, fluorescence properties can be effectively transferred to regenerated cellulosic fibers by use of fluorescence reactive dyes. These data are quite valuable for people working on new regenerated cellulose fibers and open up new perspectives for these fiber types in the development of high-visibility sportswear.