
Aramid fibers combine high specific strength, impact-energy absorption and thermal stability, yet the same rigid, highly oriented chains also produce a chemically inert surface, low compressive strength and sensitivity to ultraviolet (UV) radiation and hydrolysis. This review synthesizes original research articles, indexed in the Web of Science Core Collection, with emphasis on 2021–2026, on how fiber- and fabric-level functionalization affects the structural and functional integrity of aramid composites. Unlike previous reviews, organized by method, material form or application, it follows the retention of this integrity from fiber to component. Plasma, chemical, bio-inspired and nano structural treatments are compared by interfacial gain, fiber damage and property retention after UV exposure. The roles of aramid nanofibers, matrices, processing, hybridization and shear-thickening fluids are discussed, together with added functions such as electromagnetic shielding, strain sensing, thermal management, liquid repellence and self-healing. Several interphases, including oxide layers and aramid nanofiber coatings carrying conductive phases, strengthen adhesion while protecting the fiber or adding a function, but most data refer to unaged fibers or small specimens tested for one property at a time. An evaluation framework is proposed that links fiber, laminate and component scales with combined aging, icing and electromagnetic requirements for outdoor structures.
Fluorescence is a powerful tool to realize textile products with high-visibility effects. Fluorescent materials can transfer non-visible UV light into visible light, and by doing so, the visibility under illumination with sunlight increases. For textile products, the application of fluorescence dyes on synthetic fibers is broadly used. However, fluorescence applications are rarely reported for regenerated cellulosic fibers, such as lyocell. For this, the actual study reports on a selection of five different fluorescence dyes investigated for applications in cotton and lyocell fabrics. Dyes are considered acid dyes, basic dyes and reactive dyes, and dye application is done in increasing concentrations. Prepared textile samples are investigated according to color strength and color shade (K/S values and CIE Lab coordinates). Fluorescence emission is determined by fluorescence spectroscopy. Fastness properties are measured against rubbing, washing and light. The attained coloration increases with increased applied dye concentrations. In contrast, the achieved fluorescence emission differs strongly depending on the dye, and also, for some dye/fiber combinations with low applied dye concentration, a higher fluorescence emission is achieved. For most investigated samples, superior fluorescence effects are gained for applications in lyocell compared to simultaneously treated cotton fabrics. Especially for the investigated reactive fluorescence dyes, excellent fastness properties against rubbing, washing and light are observed. Finally, fluorescence properties can be effectively transferred to regenerated cellulosic fibers by use of fluorescence reactive dyes. These data are quite valuable for people working on new regenerated cellulose fibers and open up new perspectives for these fiber types in the development of high-visibility sportswear.
Transforming textile waste into durable, value-added materials remains a central challenge for sustainable apparel systems. This study developed single-layer, nonwoven sheets from discarded 100% cotton textiles using a papermaking-derived wet-laid process and evaluated their potential as leather-alternative materials through a sequential two-phase approach. In Phase 1, reclaimed-cotton nonwoven sheets bio-finished with persimmon juice or konjac were benchmarked against commercial plant-based olive, cork, pineapple, and cactus leather alternatives using ASTM grab tensile and rotary-platform abrasion testing. The bio-finished sheets showed low breaking forces, limited elongation, and abrasion failure. In Phase 2, biodegradable polycaprolactone (PCL) was applied as a reinforcing finish. The resulting PCL-treated reclaimed-cotton sheets’ (RC-PCL) breaking force performance improved by over 6.5 times the nontreated nonwoven specimens and approximately 4.5 times the bio-finished nonwoven specimens. Additionally, the RC-PCL completed the 2000-cycle abrasion endpoint without through-thickness failure. Elongation remained low while the dogbone tensile test showed increases in tensile strength, strain at break, and apparent Young’s modulus after PCL-finishing. These findings indicate that biodegradable PCL-finish substantially improves the strength, cohesion, and abrasion resistance of reclaimed-cotton nonwovens, while flexibility, coating optimization, and end-of-life performance remain priorities for future leather-alternative applications to support sustainability efforts and value-added use of reclaimed materials within the textile industry.
Wearables have received considerable attention due to their ability to monitor physiological and environmental data in real time. Their performance depends on innovative structures and materials that respond to diverse stimuli. A major challenge is to provide flexibility and breathability. In this context, textiles with intrinsically conducting polymers (ICPs), such as polyaniline (PANI), show great potential. This study aimed to develop a conductive material for wearable textiles through the in situ polymerization of PANI on the surface of a spacer weft-knitted fabric. Different concentrations of aniline (ANI) solution (0.05, 0.10, and 0.20 mol·L−1) were used. Analyses included thermal characterization, electrical conductivity tests, and electromechanical evaluations under compression–decompression cycles. Usability simulation tests included washing fastness, abrasion resistance, tensile strength, and perspiration tests. Samples coated using 0.10 mol·L−1 ANI exhibited the best overall performance, combining good conductivity, coating uniformity, and electromechanical stability. Morphological analyses confirmed the homogeneous deposition of PANI, while mechanical tests revealed increased tensile strength and a slight increase in material stiffness. Thermal characterization indicated slight reduction in transition temperatures associated with the presence of the polymer. Overall, the PANI-coated knitted fabric demonstrated strong potential for smart textile applications, particularly in flexible wearable textiles.
Natural fibre-reinforced polymer composites are gaining considerable attention as sustainable alternatives to fully synthetic composites because of their low density, renewability, and favourable specific mechanical properties. However, the hydrophilic nature of natural fibres can result in poor fibre–matrix adhesion and restrict composite performance. In this study, hybrid laminates were fabricated using untreated, NaOH-treated, and KMnO4-treated ramie-fibre core layers sandwiched between carbon–Kevlar intraply hybrid outer layers through hand lay-up followed by compression moulding. The laminates were evaluated using tensile, flexural, Charpy impact, and short-beam shear strength tests, while scanning electron microscopy was employed to examine interfacial bonding and fracture mechanisms. The NaOH-treated laminate exhibited the best overall mechanical performance, achieving a tensile strength of 91.62 ± 4.32 MPa, a Young’s modulus of 2.94 ± 0.21 GPa, a flexural strength of 107.78 ± 4.37 MPa, and a flexural modulus of 4.73 ± 0.45 GPa. It also recorded the highest absorbed impact energy of 1.023 J, impact strength of 38.60 kJ/m2, and short-beam shear strength of 24.17 MPa. The improvements may be associated with modifications to non-cellulosic surface constituents, potentially promoting improved fibre-matrix interaction and more efficient stress transfer. The KMnO4-treated laminate generally exhibited intermediate performance between the untreated and NaOH-treated laminates. SEM observations supported the mechanical-test results by revealing improved interfacial bonding, fewer defects, and reduced fibre pull-out in the NaOH-treated specimens. Overall, NaOH treatment was found to be the most effective surface-modification method for improving the mechanical and interfacial performance of ramie/carbon–Kevlar intraply hybrid composites intended for sustainable, lightweight structural applications.