To improve the performance and sustainability of cement mortar, this study investigates the effects of incorporating graphene oxide (GO) and metakaolin (MK) on the mechanical properties, durability performance, and microstructure of cement mortar. Among the investigated mixtures, the mortar containing 0.02 wt% GO and 3 wt% MK exhibited the best mechanical properties and durability performance. Compared with the reference mortar, the 28 d compressive and flexural strengths increased by 31.3% and 24.7%, respectively. Improvements were also observed in durability performance, including reduced water absorption, enhanced water penetration resistance, reduced drying shrinkage, and improved resistance to sulfate-induced strength deterioration. Microstructural characterization results suggested that GO may facilitate hydration product formation through nucleation effects, whereas MK consumed calcium hydroxide (Ca(OH)2) through pozzolanic reactions and contributed to the formation of additional hydration products. The incorporation of GO and MK refined the pore-size distribution and contributed to the densification of the interfacial transition zone (ITZ), thereby enhancing the mechanical properties and durability performance. These results indicate that low-dose GO combined with MK has potential for improving the mechanical properties and durability performance of cement mortar.
Inorganic permeable crystalline coatings are promising green concrete protection materials, yet the graded modification law and penetration mechanism of nano-silicon modified permeable agents on C30-C50 concrete remain unclear. This work adopts a self-developed nano-silicon super-permeable crystalline waterproofing agent, conducts surface rebound tests and single-sided salt scaling resistance tests under three coating dosages (300, 400, 500 g/m2) for C30, C40 and C50 concrete. Multi-scale characterization including SEM-EDS, XRD and MIP is performed to quantify penetration depth and microscopic pore evolution. Results show that the agent significantly improves surface hardness and salt scaling resistance of medium-low strength concrete (C30/C40): at 500 g/m2 dosage and 28 d curing, rebound strength of C30 and C40 rises by 15.06% and 9.11%, while surface scaling mass loss declines by 30.76% and 19.82%, respectively. Limited improvement is observed for C50 high-strength concrete, with only 1.31% rebound strength increment. The nano-silicon component triggers pozzolanic secondary hydration to generate abundant C-S-H gel, filling nanopores below 100 nm and refining pore structure. Stratified XRD quantification reveals penetration depths of 15 mm (C30), 10 mm (C40) and 5 mm (C50), which is linearly correlated with macroscopic performance enhancement. This study clarifies the graded penetration and modification mechanism of nano-silicon permeable materials, providing quantitative experimental basis for targeted engineering application on different strength-grade concrete structures.
Under freeze-thaw conditions, steel corrosion becomes more pronounced, leading to structural damage such as cracking, spalling, and strength reduction, which adversely affects the flexural strength, flexural-tensile strength, and freeze-thaw resistance of concrete. To address this, a study was conducted on the degradation performance of polypropylene fiber-reinforced concrete considering steel corrosion during freeze-thaw cycles. Polypropylene fiber-reinforced concrete was prepared by mixing pretreated polypropylene fibers with cement and other admixtures. The flexural strength, flexural-tensile strength, and elastic modulus of polypropylene fiber-reinforced concrete with fiber contents of 0.2%, 0.4%, and 0.6% were tested before and after corrosion and under different numbers of freeze-thaw cycles. The experimental results indicate that, compared with plain concrete, the polypropylene fiber-reinforced concrete exhibited less degradation under freeze-thaw cycles and corrosion, exhibiting reduced surface damage and mass loss. The flexural strength and flexural-tensile strength of concrete with 0.2% polypropylene fiber were lower than those with 0.6% polypropylene fiber, and the elastic modulus test results were also inferior. The performance of concrete with 0.4% polypropylene fiber was moderate. Comprehensive analysis demonstrates that polypropylene fiber-reinforced concrete with a 0.6% fiber content exhibited the least deterioration in freeze-thaw damage after corrosion in salt solution.
Rubberized geopolymer concrete (RuGC) is a novel material that combines the environmental and durability benefits of geopolymer concrete (GC) with the flexibility and energy absorption capabilities of rubber aggregates. This hybrid material holds strong potential for structural applications where enhanced tensile strength and impact resistance are desirable. However, its mechanical performance under various loading conditions remains insufficiently explored. In this study, the mechanical behavior of RuGC was evaluated through an experimental program in which aggregates were partially replaced with rubber aggregates at replacement levels of 5%, 10%, and 15%. Experiments were conducted to assess compressive strength, tensile strength, and load-bearing capacity, while the influence of rubber content and curing conditions on mechanical performance was systematically examined. The results indicate that incorporating 10% fine crumb rubber and 5% coarse crumb rubber caused only a marginal reduction in mechanical properties while maintaining satisfactory structural behaviour. These findings highlight RuGC as a promising construction material capable of reducing both rubber waste and the carbon footprint associated with traditional concrete production.
Incorporating phase change materials (PCMs) into cementitious composites enhances latent heat storage but generally compromises mechanical performance. This study investigates the combined effects of microencapsulated tetradecane (m-PCM), incorporated at 5% and 10% by weight of cement, and 0.10 wt.% multiwalled carbon nanotubes (MWCNTs) on a high-strength cementitious composite (HSCC) for low-temperature thermal energy storage. Encapsulation increased the onset temperature of thermal degradation from 144.5 degrees C to 226.9 degrees C, while the m-PCM exhibited crystallization and melting enthalpies of 251.5 and 84.76 J/g, respectively. Relative to the 28-day reference strength of 119.83 MPa, m-PCM reduced compressive strength by 17.3% and 33.4%, whereas MWCNT incorporation mitigated these reductions to 12.6% and 18.3%. During five thermal cycles between -5 degrees C and 15 degrees C, the minimum internal temperature increased from -2.0 degrees C for MPCM5% to -0.8 degrees C for MPCM10% and -0.1 degrees C for MPCM10%C. SEM-EDS and XRD indicated localized hydration retardation and a dilution effect associated with m-PCM incorporation. MPCM10%C exhibited the best thermal response while retaining a 28-day compressive strength of 97.92 MPa, demonstrating its potential for high-strength structuralfunctional cementitious composites with low-temperature thermal energy storage capability.