Ensuring the long-term chemical durability of glasses is critical for nuclear waste immobilization operations. Durable glasses usually undergo qualification for disposal based on their response to standardized tests such as the product consistency test or the vapor hydration test (VHT). The VHT uses elevated temperature and water vapor to accelerate glass alteration and the formation of secondary phases. Understanding the relationship between glass composition and VHT response is of fundamental and practical interest. However, this relationship is complex, non-linear, and sometimes fairly variable, posing challenges in identifying the distinct effect of individual oxides on VHT response. Here, we leverage a dataset comprising 654 Hanford low-activity waste (LAW) glasses across a wide compositional envelope and employ various machine learning techniques to explore this relationship. We find that Gaussian process regression (GPR), a non-parametric regression method, yields the highest predictive accuracy. By utilizing the trained model, we discern the influence of each oxide on the glasses' VHT response. Moreover, we discuss the trade-off between underfitting and overfitting for extrapolating the material performance in the context of sparse and heterogeneous datasets.
The 2018 Camp Fire was a large late-year (November) wildfire that produced an urban firestorm in the Town of Paradise, California, USA, and destroyed more than 18 000 structures. Runoff from burned wildland areas is known to contain ash, which can transport contaminants including metals into nearby watersheds. However, due to historically infrequent occurrences, the effect of wildland-urban interface (WUI) fires, such as the Camp Fire, on surface water quality has not been well-characterized. Therefore, this study investigated the effects of widespread urban burning on surface water quality in major watersheds of the Camp Fire area. Between November 2018 and May 2019, 140 surface water samples were collected, including baseflow and stormflow, from burned and unburned watersheds with varying extent of urban development. Samples were analyzed for total and filter-passing metals, dissolved organic carbon, major anions, and total suspended solids. Ash and debris from the Camp Fire contributed metals to downstream watersheds via runoff throughout the storm season. Increases in concentration up to 200-fold were found for metals Cr, Cu, Ni, Pb, and Zn in burned watersheds compared to pre-fire values. Total concentrations of Al, Cd, Cu, Pb, and Zn exceeded EPA aquatic habitat acute criteria by up to 16-fold for up to five months after the fire. To assess possible transport mechanisms and bioavailability, a subset of 18 samples was analyzed using four filters with nominal pore sizes ranging from 0.22 to 1.2 mu m to determine the particulate size distribution of metals. Trace and major metals (Al, Ba, Co, Cr, Cu, Fe, Hg, Mn, Ni, Pb, and Zn) were found mostly associated with larger grain sizes (>0.45 mu m), and some metals (Al, Cr, Fe, and Pb) also included a substantial colloidal phase (0.22 to 0.45 mu m). This study suggests that fires in the wildland-urban interface increase metal concentrations, mainly through particulate driven transport. The metals with the largest increases are likely from anthropogenic disaster materials, though biomass ash also is a major contributor to water quality. The increase in metals following WUI burning may have adverse ecological impacts.
The DOE Office of Environmental Management is responsible for high level nuclear waste that must be safely isolated from humans and the environment for extremely long periods. The waste forms and containers are made of glass, ceramics, and metals. Verified safe disposal requires understanding the fundamental mechanisms of waste form degradation and the design of new waste forms with improved performance, which comprise the goals of the Energy Frontier Research Center known as the Center for the Performance and Design of Nuclear Waste Forms and Containers, WastePD. WastePD was constructed to develop innovative approaches and solutions to those goals through the synergistic interactions of individuals who are experts in the degradation behavior, modeling, and design of glasses, ceramics and metal alloys. WastePD is the first center ever created to address this diverse group of materials in a comprehensive and coordinated manner. The science goals are grouped into three common topics: corrosion mechanisms via advanced characterization, environmental impacts, and materials design. Synergistic interactions in these areas were a key component of WastePD. The fundamental understanding of the degradation mechanisms of the waste forms and containers as well as the development of new materials with improved properties will allow DOE to prevent environmental contamination and to explore totally new repository concepts. WastePD was operational from August 2016 through July 2022, but the DOE support was drastically reduced for the last two years. This final technical report covers the full period of performance. However, much of what was accomplished in the first four years is nicely summarized in a review paper published in 2021, which is appended to this report. Therefore, this final report focuses on the technical findings from the last two years of WastePD activities. Considerable progress was made in the areas of a) the environmental and compositional impacts on the corrosion of borosilicate and aluminosilicate glasses, b) the mechanism of glass corrosion and the structure and evolution of the surface alteration layer, c) the effects of environment and composition on the corrosion of pyrochlore, perovskite, hollandite, and other oxide ceramics, d) the corrosion mechanism of multi-principal element metallic alloys, and e) a new framework for understanding the pitting corrosion of metals.
Predicting the chemical durability of glass materials is important for various applications from daily life such as cell phone screens and kitchenware to advanced technologies such as nuclear waste disposal and biomedicine. In this work, we explored the prediction of the initial glass dissolution rates using structural features from molecular dynamics (MD) simulations for a series of glass compositions (total 28), including ZrO2- and V2O5-containing boroaluminosilicate, borosilicate, and aluminosilicate glasses. The initial dissolution rates (r(0)) measured experimentally at 90 degrees C with varying solution conditions were correlated with structural features (e.g., polyhedral linkages and non-bridging oxygen species) obtained from MD simulations, either from this study or from literature. As hydrolysis of the glass network through breaking of the network former linkages (e.g., Si-O-Si, Si-O-Al, etc.) is a critical step of network glass dissolution, the statistics of these linkages obtained from MD were also correlated to r(0) through linear regression, where the coefficients of determination (R-2) and root mean square error are found to be 0.949 and 0.681, respectively. This model was compared and discussed with existing models developed by various approaches, including machine learning, the kinetic rate equation, topological constraint theory, and other descriptors from MD simulations. The discussion provides insights on future model improvements to predict glass dissolution. In addition, as the effect of V2O5 on glass dissolution was not well studied comparing to ZrO2, the impact of V2O5 was emphasized in this paper, suggesting that the impact is not the same across all glass compositions and test conditions.
Given the importance of glass materials to society, their durability when exposed to aqueous solutions is a critical area for research, particularly for vitrified radioactive wastes. This spurred an international team to fabricate a standardized composition based on waste immobilization glass called the International Simple Glass (ISG), which has been the subject of numerous experimental and computational studies focused on aqueous corrosion resistance. With the original batch of ISG nearly depleted, the international team designed and fabricated a standard glass material, ISG-2, where half the Ca in the original composition was replaced with Mg by mole. This paper presents information on both the ISG-2 composition and a new batch with the same nominal composition as the original ISG, designated ISG-1, including their homogeneity, their physical and thermal properties. The results of static alteration experiments are presented as well to provide a baseline for future aqueous corrosion performance investigations.
Long-term laboratory-scale static alteration tests (up to 1500 d) were conducted on two low-activity waste glasses (LAWA44 and IDF18-A161) at S/V = 2000 m(-1). Tests were seeded with either analcime, clinoptilolite, zeolite P1, or zeolite P2 to induce Stage III glass alteration behavior. The effect of several parameters on glass Stage III behavior was studied with consideration of several variables, including temperature (22 degrees C-90 degrees C) and pH (floating or initially set using KOH at values from 9.5 to 11.5). Temporal solution data and solids characterization at the end of the experiments are reported. Solution data demonstrated the occurrence of a sustained rate acceleration at temperatures down to 40 degrees C and the activation energy for these Stage III rates was determined for both glasses. Three major secondary phases were identified at the end of the experiments for both glasses: zeolite P1, zeolite P2, and/or analcime (along with minor phases: zeolites, clays, carbonates). The identity of the crystalline phases at the end of the experiment often differed from the zeolite seed phase. In addition, the use of the Avrami equation showed unimpeded zeolite growth (3-dimensional) in certain conditions, suggesting that in certain conditions the glass dissolution rate is controlled by zeolite formation kinetics whereas in other conditions the glass corrosion process impeded zeolite formation kinetics. The morphological evolution of the samples revealed the growth of the zeolites which completely fill the intergranular space in the powder bed. These results are discussed with regards to previous seeded and unseeded Stage III dissolution rate experiments performed on low- and high-activity nuclear waste glasses. (c) 2022ElsevierB.V. Allrightsreserved.
An understanding of the mechanisms responsible for controlling the long-term corrosion rate of nuclear waste glass is paramount if reliable glass dissolution models are to be used to calculate the controlled release of radionuclides from nuclear waste glass under geologic disposal conditions. Understanding the mechanism that controls silicate glass dissolution rates is also important for natural glasses to understand the role from the dissolution of these glasses has on the composition of natural aquatic systems. Two general mechanisms appear to be responsible for the elemental release from glass to the surrounding biosphere – ion exchange (release principally of alkalis) and matrix dissolution (release of the structural components of the glass). Key unknowns related to these mechanisms are the impact of surface layers on the altered glass and how these layers participate in corrosion. To better understand the impact of these layers on the long-term glass corrosion rate, we made two glasses of the same elemental composition, but with selected elements enriched in specific isotopes for B (11B), Li (6Li), and Si (29Si). We reacted these glasses for 1 y then the solutions from each were exchanged and the chemistry of the solutions and the solids were followed for another 2 y (a total of 3 y). This allowed us to follow changes in the glasses with respect to these elements and how these elements were transported through the alteration layers with time and, for at least one element, into the glass and to deconvolute some competing kinetic steps, such as matrix dissolution and ion exchange. Results from these experiments demonstrate that the release behavior of different elements is strongly dependent on their structural role in the glass (e.g. network formers and modifiers), but, more importantly, the role of water transport and subsequent ion exchange has in the long-term dissolution of the glass studied here. In this article, we highlight the behavior of four elements: lithium, sodium, silicon, and boron. Lithium and sodium, network modifying elements, have similar chemistries. The behavior of Li could be tracked in more detail by following both 6Li and 7Li; Li penetrates through the gel layer in both directions without hinderance and is released from the glass deeper than Na. Silicon, a network forming element, reacts with the silica-rich alteration layer. Boron, a network forming element, does not accumulate in the gel or the pristine glass and has a very sharp elemental profile between the pristine glass and alteration layer. Boron, lithium, and sodium elemental profiles suggest that there is little if any transport control within the alteration layer. These results are similar to those found for basalt glass. However, the correlation between the Li and Na profiles and that of a water species suggest that the limiting release is not controlled by the formation of the gel but rather is a steady state between the diffusion of a water species and matrix dissolution that results in a low release rate for alkali and this provides a steady driving force for the long-term dissolution of glass.
This project aimed to gain detailed and fundamental understanding of the stability of glass waste forms to be used for safe and reliable encapsulation of nuclear waste. The focus was to understand thermodynamic and structural properties involved in crystallization and phase separation in melt-derived waste form glasses and glass-ceramics by studying a baseline glass composition with varying additives. This was achieved by combining neutron total scattering, advanced calorimetric measurements, and extensive modeling study. This project harnessed diverse and complementary approaches and expertise from four collaborating interdisciplinary institutions (two universities, one national laboratory, and one UK university partner). Samples were prepared at the national laboratory and exchanged with the two university institutions. The thermodynamic data obtained by various advanced calorimetry techniques were linked to the underlying short-range structure of waste forms measured by state-of-the-art neutron total scattering experiments. An important element of this project was extensive modeling to interpret and fundamentally understand the experimental results.
Fluids leaked from oil and gas wells often originate from their surface casing─a steel pipe installed beneath the deepest underlying source of potable groundwater that serves as the final barrier around the well system. In this study, we analyze a regulatory dataset of surface casing geochemical samples collected from 2573 wells in northeastern Colorado─the only known publicly available dataset of its kind. Thermogenic gas was present in the surface casings of 96.2% of wells with gas samples. Regulatory records indicate that 73.3% of these wells were constructed to isolate the formation from which the gas originated with cement. This suggests that gas migration into the surface casing annulus predominantly occurs through compromised barriers (e.g., steel casings or cement seals), indicative of extensive integrity issues in the region. Water was collected from 22.6% of sampled surface casings. Benzene, toluene, ethylbenzene, and xylenes were detected in 99.7% of surface casing water samples tested for these compounds, which may be due to the presence of leaked oil, natural gas condensate, or oil-based drilling mud. Our findings demonstrate the value of incorporating surface casing geochemical analysis in well integrity monitoring programs to identify integrity issues and focus leak mitigation efforts.
The San Joaquin Valley (SJV) in California is one of the most agriculturally productive regions in the world relying in part on groundwater for irrigation and for domestic or municipal water supply for nearly 4 million residents. One area of growing concern in the SJV is potential impact to groundwater resources from ongoing and historical disposal of oilfield-produced water into unlined produced water ponds (PWPs). In this investigation, we utilized available information on composition of produced water disposed into unlined PWPs and levels of total dissolved solids in underlying groundwater to demonstrate that this disposal practice, both past and present, poses risks to groundwater resources, especially in the Tulare Basin in the southern SJV. Groundwater monitoring at unlined PWP facilities is relatively sparse, but where monitoring has occurred, impact to aquifers used for public and agricultural water supply has been observed and has proven to be too expensive to actively remediate. Results of this investigation should inform policy discussions in California and other locations where disposal of produced water into unlined impoundments occurs, especially at locations that overlie groundwater resources.
Oil and gas wells with compromised integrity are a concern because they can potentially leak hydrocarbons or other fluids into groundwater and/or the atmosphere. Most states in the United States require some form of integrity testing, but few jurisdictions mandate widespread testing and open reporting on a scale informative for leakage risk assessment. In this study, we searched 33 US state oil and gas regulatory agency databases and identified records useful for evaluating well integrity in Colorado, New Mexico, and Pennsylvania. In total, we compiled 474,621 testing records from 105,031 wells across these states into a uniform dataset. We found that 14.1% of wells tested prior to 2018 in Pennsylvania exhibited sustained casing pressure (SCP) or casing vent flow (CVF)-two indicators of compromised well integrity. Data from different hydrocarbon-producing regions within Colorado and NewMexico revealed a wider range (0.3 to 26.5%) of SCP and/or CVF occurrence than previously reported, highlighting the need to better understand regional trends in well integrity. Directional wells were more likely to exhibit SCP and/or CVF than vertical wells in Colorado and Pennsylvania, and their installation corresponded with statewide increases in SCP and/or CVF occurrence in Colorado (2005 to 2009) and Pennsylvania (2007 to 2011). Testing the ground around wells for indicators of gas leakage is not a widespread practice in the states considered. However, 3.0% of Colorado wells tested and 0.1% of New Mexico wells tested exhibited a degree of SCP sufficient to potentially induce leakage outside the well.
High-level radioactive waste is accumulating at temporary storage locations around the world and will eventually be placed in deep geological repositories. The waste forms and containers will be constructed from glass, crystalline ceramic, and metallic materials, which will eventually come into contact with water, considering that the period of performance required to allow sufficient decay of dangerous radionuclides is on the order of 105-106 years. Corrosion of the containers and waste forms in the aqueous repository environment is therefore a concern. This Review describes the recent advances of the field of materials corrosion that are relevant to fundamental materials science issues associated with the long-term performance assessment and the design of materials with improved performance, where performance is defined as resistance to aqueous corrosion. Glass, crystalline ceramics, and metals are discussed separately, and the near-field interactions of these different material classes are also briefly addressed. Finally, recommendations for future directions of study are provided.
The presence of methane and other hydrocarbons in domestic-use groundwater aquifers poses significant environmental and human health concerns. Isotopic measurements are often relied upon as indicators of groundwater aquifer contamination with methane. While these parameters are used to infer microbial metabolisms, there is growing evidence that isotopes present an incomplete picture of subsurface microbial processes. This study examined the relationships between microbiology and chemistry in groundwater wells located in the Denver-Julesburg Basin of Colorado, a rapidly urbanizing area with active oil and gas development. A primary goal was to determine if microbial data can reliably indicate the quantities and sources of groundwater methane. Comprehensive chemical and molecular analyses were performed on 39 groundwater well samples from five aquifers. Elevated methane concentrations were found in only one aquifer, and both isotopic and microbial data support a microbial origin. Microbial parameters had similar explanatory power as chemical parameters for predicting sample methane concentrations. Furthermore, a subset of samples with unique microbiology corresponded with unique chemical signatures that may be useful indicators of methane gas migration, potentially from nearby coal seams interacting with the aquifer. Microbial data may allow for more accurate determination of groundwater contamination and improved long-term water quality monitoring compared solely to isotopic and chemical data in areas with microbial methane.
Vanadium-containing glasses have aroused interest in several fields such as electrodes for energy storage, semiconducting glasses, and nuclear waste disposal. The addition of V2O5, even in small amounts, can greatly alter the physical properties and chemical durability of glasses; however, the structural role of vanadium in these multicomponent glasses and the structural origins of these property changes are still poorly understood. We present a comprehensive study that integrates advanced characterizations and atomistic simulations to understand the composition-structure-property relationships of a series of vanadium-containing aluminoborosilicate glasses. UV-vis spectroscopy, X-ray photoelectron spectroscopy, and X-ray absorption near-edge structure (XANES) have been used to investigate the complex distribution of vanadium oxidation states as a function of composition in a series of six-component aluminoborosilicate glasses. High-energy X-ray diffraction and molecular dynamics simulations were performed to extract the detailed short- and medium-range atomistic structural information such as bond distance, coordination number, bond angle, and network connectivity, based on recently developed vanadium potential parameters. It was found that vanadium mainly exists in two oxidation states: V5+ and V4+, with the former being dominant (∼80% from XANES) in most compositions. V5+ ions were found to exist in 4-, 5-, and 6-fold coordination, while V4+ ions were mainly in 4-fold coordination. The percentage of 4-fold-coordinated boron and network connectivity initially increased with increasing V2O5 up to around 5 mol % but then decreased with higher V2O5 contents. The structural role of vanadium and the effect on glass structure and properties are discussed, providing insights into future studies of sophisticated structural descriptors to predict glass properties from composition and/or structure and aiding the formulation of borosilicate glasses for nuclear waste disposal and other applications.
The dissolution rate of some glasses accelerates after prolonged time spent at a slow, residual dissolution rate. This phenomenon is referred to as Stage III behavior. The acceleration in glass dissolution rate linked to Stage III behavior is significant and may be the most impactful behavior to long-term performance of glass in a repository. This work is aimed at understanding the effect of glass composition on Stage III behavior to add a level of technical defensibility to glass disposal. To this end, a set of 24 glass compositions were statistically designed, where eight glass components (SiO2, B2O3, Al2O3, CaO, Na2O, SnO2, ZrO2, and Others) have been independently varied in order to study the individual effects of each glass component. These glasses have been subjected to static dissolution tests at 90 degrees C in deionized water and then seeded with zeolite Na-P2 28 days into the testing to induce Stage III behavior. The response of the glasses to the zeolite seeds fell into four primary types: (1) no response to seeds; (2) an immediate linear sustained acceleration in the rate; (3) an immediate linear acceleration in the rate followed by a decrease; and (4) a progressive acceleration in the rate that is concurrent with the addition of the seeds. The main glass components observed to influence these behaviors were CaO, Al2O3, B2O3, and ZrO2, where (1) CaO influenced which glasses showed a Stage III response to seeds (high CaO: types 2, 3, and 4) or did not respond to seeds (low CaO: type 1), (2) Al2O3 and B2O3 influenced which glasses showed a sustainable Stage III response (high Al2O3: types 2 and 4) versus transitory response (low Al2O3 and high B2O3: type 3), and (3) ZrO2 concentration influenced whether glasses showed a linear (high ZrO2: type 2) versus progressive (low ZrO2: type 4) response to seeds.
Mining provides significant economic value while often impacting local water supplies and environments because of freshwater usage and waste disposal practices. This study identifies current practices in mine water, including how water is used in mining, influent and effluent water quality, treatment technologies, and end uses with the goal of informing future research on implementable, reliable, and cost-effective advanced water treatment in the mining sector. This study also reviews the available literature to broadly evaluate mining in the United States and performs a techno-economic assessment on water use and disposal for three detailed case studies applicable to lithium, uranium, and copper mines. These case studies highlight specific industry examples of distinct extraction methods, geographical regions, and mined commodities. Hypothetical scenarios based on case study baselines revealed potential impacts to mine water available for beneficial reuse through the use of novel water treatment technologies and alternate water management strategies. Finally, an assessment of national level impacts resulting from the reuse of treated mine source water is presented.
The nanoscale microstructure and chemistry of a transparent gahnite glass-ceramic and its precursor glass were investigated using atom probe tomography, transmission electron microscopy, and nuclear magnetic resonance spectroscopy. In the annealed precursor glass, statistically significant ZrO clustering was observed along with Si depletion within 2 nm of the ZrO clusters. This clustering is expected to be the first step in the nucleation and crystallization of the nucleating agent, ZrO2. In the glass-ceramic, gahnite (ZnAl2O4) crystallites were found to exist in proximal locations to ZrO2 and not in a core-shell arrangement. The residual glass composition was directly measured by atom probe, showing higher concentrations of Al, Zn, and Zr than previously expected. At the interfaces between the crystallites and residual glass, no enrichment or depletion zones were found. These findings provide answers to outstanding questions surrounding the nucleation and elemental partitioning, microstructure, and the residual glass composition of transparent gahnite glass-ceramics.