Ultra-high-performance concrete (UHPC) enables thinner, longer- span elements with fewer or no reinforcing bars. This study investigates the shear behavior of reinforcing bar-free UHPC panels with a thickness of 4 in. (101.6 mm) and 2.0% volumetric content of straight steel fibers. The panels were tested under combined shear and axial loads using the universal panel tester (UPT) facility. The UPT experiments were complemented with small-scale direct tension tests (DTTs) and large-scale tension strip tests (TSTs) to investigate the effect of UHPC tensile characteristics on shear. The panels exhibited ductile responses with post-peak residual shear capacities higher than 20% of the maximum shear stress, with the TSTs providing an improved correlation to UHPC shear than the DTTs. Test results showed that the relative effect of axial loads on UHPC shear can be greater than the relative effect on conventional concrete per ACI 318. It was also found that a correlation exists between fiber alignment and UHPCs' tensile behavior, which can alter the localization stress by as much as 39%.
A waterborne topcoat had been spray-applied to the underside of a factory-primed galvanized steel deck at an exterior, sheltered location of a shipment station. After nine months, extensive intercoat delamination failure occurred. The root cause of the poor intercoat adhesion was investigated by onsite inspections, review of project documents, and laboratory testing. Infrared spectroscopical analyses were additionally employed to characterize the factory-applied deck primer and to understand its role in the delamination failures. As part of the investigation, five different topcoat products were applied to samples of factory-primed decking. The coating adhesion of these trial specimens was measured and evaluated. The investigation ultimately revealed the use of a topcoat incompatible with the factory-applied deck primer. The results of the investigation were utilized to develop an approach for successful future painting of the factory-applied deck primer.
Bridge decks exposed to de-icing agents and marine environments often deteriorate due to chloride-induced corrosion. Investigations characterizing current condition and expected future durability are critical to facilitating appropriate selection and timing of rehabilitation actions. These investigations can be most effective if based on thorough field assessments supported by probabilistic service life modeling. Two such investigations of reinforced concrete bridge decks, located in the Midwest-Region of the United States, are presented as case studies; one located in Indiana and another in Illinois. For each case study, field assessment and material testing were performed in the early 2010’s, and then a follow-up assessment was performed in the early 2020’s (studies performed roughly ten years apart). The investigations included evaluations of changes in chloride contamination at the surface and through the cover concrete, and of damage propagation rates relative to field measurements. The findings show that chloride diffusion modeling is an effective tool for predicting chloride ingress and associated damage rates. The findings also highlight the importance of characterizing variability in bridge conditions during modeling efforts.
Reddish-brown staining appeared on pre-primed steel framing members soon after the application of the topcoat. Despite the primer manufacturer’s early hypothesis that surfactant leaching of the topcoat may have been the cause, field and laboratory investigations indicated that water-soluble corrosion products were being mobilized and deposited on the surface due to the presence of moisture. Pre-primed steel delivered to jobsites can begin to rust before receiving the topcoat. Areas of latent corrosion where the primer thickness was low, along with the framing that had been stored outdoors, likely led to corrosion staining after topcoat application.
Following the 2011 downtown Christchurch earthquake, 60% of buildings in Christchurch were demolished and reconstructed. Such practices are costly in terms of money and carbon emissions. Structures need to be proportioned so that they can be reused after one or several ground motions. To do so, it is important to understand the effect of previous shaking on drift demands. Past studies conducted to investigate the effect of previous shaking were based almost exclusively on numerical analyses that used a limited set of parameters. Conclusions from past numerical analyses do not lead to a clear consensus, and results from past studies have not been systematically vetted against measurements from structures tested in the laboratory or evidence from the field. To address these issues, the plausible effects of previous shaking on drift demands were re-evaluated using (1) numerical analyses of Single and Multi-Degree-of-Freedom oscillators with an expanded set of parameters and (2) measurements from 220 experimental tests of structures subjected to repeated simulated base motions. The compiled evidence supports at least two conclusions: (1) Repeats of medium or high-intensity motions strong enough to cause yielding in their first occurrence are unlikely to produce large relative increases in peak drift demands in structures with stable force–displacement relationships not susceptible to brittle failures. This phenomenon was observed in repeated motions not preceded by more intense motions, as well as in repeated motions preceded by more intense motions. The latter observation had not been reported in the literature to date. (2) Increases in peak drift demands were observed to be likely to occur if the first motion (in a sequence of motions containing a pair of repeated motions) is mild enough not to cause cracking and/or yielding, but the second instance of the same motion is preceded by larger intensity motions causing cracking and/or yielding.